A Bioinspired Surface with Synergistic Effect of Anisotropy and Gradient Microstructures for Controllable Fluid Transportation AITranslate

Dalian Maritime University; Dalian Maritime University; Dalian Maritime University; Dalian Maritime University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The fluid on micro-nanostructures with anisotropy or gradient can exhibit highly inducible wettability that can be found in both nature and artificiality. In this study, inspired by the anisotropic and gradient micro-nanostructures on rice leaf and cactus spine, respectively, we fabricated a wedgy polydimethylsiloxane with ordered micropit arrays (WPOMA) by a rapid strategy to strengthen the property of directional water transportation as a result of their synergistic effect. The unit structure in the array exhibits anisotropy under stretched stress, whereas the unit structure in the long range along the WPOMA shows an arrangement of gradient. Therein, the anisotropic elliptical micropit arrays generated by stretched stress contribute to the axial flow, whereas the gradual change of micropit arrays with morphology gradient contributes to the directional flow. The concurrent axial and directional flows have a great performance in fluid transportation and collection. Additionally, the anisotropic and gradient synergistic micro-nanostructures can be controlled in real time by reversible mechanical stress, which was revealed at the stretched state and hidden at the released state. Meanwhile, the flexible texture effectuated the flow-induced capacity even at the bending state. On the basis of the synergistic effect and switchable wettability, the flexible material paves a way in the potential applications in anti-drag wearable devices, droplet manipulators, and controllable fluid transportation.

KeyWords AITranslate

anisotropy gradient synergistic effect fluid transportation switchable
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02119

Chinese Library Classification Number:

Citation Information:

The fluid on micro-nanostructures with anisotropy or gradient can exhibit highly inducible wettability that can be found in both nature and artificiality. In this study, inspired by the anisotropic and gradient micro-nanostructures on rice leaf and cactus spine, respectively, we fabricated a wedgy polydimethylsiloxane with ordered micropit arrays (WPOMA) by a rapid strategy to strengthen the property of directional water transportation as a result of their synergistic effect. The unit structure in the array exhibits anisotropy under stretched stress, whereas the unit structure in the long range along the WPOMA shows an arrangement of gradient. Therein, the anisotropic elliptical micropit arrays generated by stretched stress contribute to the axial flow, whereas the gradual change of micropit arrays with morphology gradient contributes to the directional flow. The concurrent axial and directional flows have a great performance in fluid transportation and collection. Additionally, the anisotropic and gradient synergistic micro-nanostructures can be controlled in real time by reversible mechanical stress, which was revealed at the stretched state and hidden at the released state. Meanwhile, the flexible texture effectuated the flow-induced capacity even at the bending state. On the basis of the synergistic effect and switchable wettability, the flexible material paves a way in the potential applications in anti-drag wearable devices, droplet manipulators, and controllable fluid transportation.

quote

GB/T 7714-2015 [1] Kai Sheng, Peihong Xue, Hao Liu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02119.
MLA [1] Kai Sheng, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02119.
APA [1] Kai Sheng, Peihong Xue, Hao Liu, & Xiwei Wang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02119
IEEE [1] Kai Sheng, Peihong Xue, Hao Liu, and Xiwei Wang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02119. keywords: {anisotropy;gradient;synergistic effect;fluid transportation;switchable}