Influence of Trimethylsilyl Side Groups on the Molecular Mobility and Charge Transport in Highly Permeable Glassy Polynorbornenes AITranslate

Bundesanstalt für Materialforschung und−prüfung (BAM), Unter den Eichen 87;A.V. Topchiev Institute of Petrochemical Synthesis of Russian Academy of Science;A.V. Topchiev Institute of Petrochemical Synthesis of Russian Academy of Science;Bundesanstalt für Materialforschung und−prüfung (BAM), Unter den Eichen 87;Bundesanstalt für Materialforschung und−prüfung (BAM), Unter den Eichen 87;Bundesanstalt für Materialforschung und−prüfung (BAM), Unter den Eichen 87
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Superglassy polymers with a large fractional free volume have emerged as novel materials with a broad range of applications, especially in the field of membrane separations. Highly permeable addition-type substituted polynorbornenes with high thermal resistance and chemical stability are among the most promising materials. The major obstacle for extending the practical membrane application is their strong tendency to physical aging, leading to a partial decline in their superior transport performance over time. In the present study, broadband dielectric spectroscopy with complementary X-ray scattering techniques were employed to reveal changes in microporous structure, molecular mobility, and conductivity by systematic comparison of two polynorbornenes with different numbers of trimethylsilyl side groups. Their response upon heating (aging) was compared in terms of structure, dynamics, and charge transport behavior. Furthermore, a detailed analysis of the observed Maxwell–Wagner–Sillars polarization at internal interfaces provides unique information about the microporous structure in the solid films. The knowledge obtained from the experiments will guide and unlock potential in synthesizing addition-type polynorbornenes with versatile properties.

KeyWords AITranslate

polynorbornene dielectric spectroscopy molecular mobility conductivity gas separation membranes
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00092

Chinese Library Classification Number:

Citation Information:

Superglassy polymers with a large fractional free volume have emerged as novel materials with a broad range of applications, especially in the field of membrane separations. Highly permeable addition-type substituted polynorbornenes with high thermal resistance and chemical stability are among the most promising materials. The major obstacle for extending the practical membrane application is their strong tendency to physical aging, leading to a partial decline in their superior transport performance over time. In the present study, broadband dielectric spectroscopy with complementary X-ray scattering techniques were employed to reveal changes in microporous structure, molecular mobility, and conductivity by systematic comparison of two polynorbornenes with different numbers of trimethylsilyl side groups. Their response upon heating (aging) was compared in terms of structure, dynamics, and charge transport behavior. Furthermore, a detailed analysis of the observed Maxwell–Wagner–Sillars polarization at internal interfaces provides unique information about the microporous structure in the solid films. The knowledge obtained from the experiments will guide and unlock potential in synthesizing addition-type polynorbornenes with versatile properties.

quote

GB/T 7714-2015 [1] Huajie Yin, Pavel Chapala, Maxim Bermeshev, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00092.
MLA [1] Huajie Yin, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00092.
APA [1] Huajie Yin, Pavel Chapala, Maxim Bermeshev, Brian R. Pauw, Andreas Schönhals, & Martin Böhning. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00092
IEEE [1] Huajie Yin, Pavel Chapala, Maxim Bermeshev, Brian R. Pauw, Andreas Schönhals, and Martin Böhning, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00092. keywords: {polynorbornene;dielectric spectroscopy;molecular mobility;conductivity;gas separation membranes}