daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Facile Approach for the Preparation of Robust and Thermally Stable Silyl Ether Cross-Linked Poly(ethylene-vinyl acetate) Vitrimers AITranslate

Dalian Polytechnic University;Dalian Polytechnic University; Dalian Institute of Chemical Physics;Petrochemical Research Institute;Petrochemical Research Institute;Dalian Polytechnic University; Dalian Institute of Chemical Physics; Dalian Institute of Chemical Physics
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vitrimers as an emerging class of dynamic polymer networks hold great promise for the development of sustainable thermosets. While the straightforward method to prepare vitrimers from commodity polymers is cost-competitive, most studies involved the synthesis of polymers with specific functional groups and/or crosslinkers. Herein, we demonstrated a simple and scalable approach to produce poly(ethylene-vinyl acetate) (EVA) vitrimers by direct cross-linking of an industrial EVA product with commercial bis[3-(trimethoxysilyl)propyl]amine using titanium(IV) butoxide as a catalyst through reactive blending. Incorporation of the thermally stable silyl ether cross-links into the network led to significantly enhanced thermal and mechanical properties. Compared to the original EVA, the resulting vitrimers showed up to 4 and 2 times improvement in Young’s modulus and tensile strength, respectively. The creep resistance of the EVA vitrimer increased with the cross-linking density, and notably, EVA-V0.8 displayed a low permanent deformation of 1.2% at a high temperature of 180 °C, much higher than the normal service temperature. Moreover, the vitrimers displayed excellent reprocessability and recyclability, and the Young’s modulus, tensile strength, and elongation at break of the EVA vitrimers were nearly identical even after four times of recycling.

KeyWords AITranslate

polyolefin reactive blending vitrimer silyl ether creep resistance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01516

Chinese Library Classification Number:

Citation Information:

Vitrimers as an emerging class of dynamic polymer networks hold great promise for the development of sustainable thermosets. While the straightforward method to prepare vitrimers from commodity polymers is cost-competitive, most studies involved the synthesis of polymers with specific functional groups and/or crosslinkers. Herein, we demonstrated a simple and scalable approach to produce poly(ethylene-vinyl acetate) (EVA) vitrimers by direct cross-linking of an industrial EVA product with commercial bis[3-(trimethoxysilyl)propyl]amine using titanium(IV) butoxide as a catalyst through reactive blending. Incorporation of the thermally stable silyl ether cross-links into the network led to significantly enhanced thermal and mechanical properties. Compared to the original EVA, the resulting vitrimers showed up to 4 and 2 times improvement in Young’s modulus and tensile strength, respectively. The creep resistance of the EVA vitrimer increased with the cross-linking density, and notably, EVA-V0.8 displayed a low permanent deformation of 1.2% at a high temperature of 180 °C, much higher than the normal service temperature. Moreover, the vitrimers displayed excellent reprocessability and recyclability, and the Young’s modulus, tensile strength, and elongation at break of the EVA vitrimers were nearly identical even after four times of recycling.

quote

GB/T 7714-2015 [1] Jincheng Zhang, Xiaopei Li, Songbo Zhang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01516.
MLA [1] Jincheng Zhang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01516.
APA [1] Jincheng Zhang, Xiaopei Li, Songbo Zhang, Wenqin Zhu, Shuanhong Li, Yongjie Zhang, Yanming Hu, & Guangyuan Zhou. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01516