Self-Stratified Coating with Multiresponsive Self-Healing Polymer AITranslate
Abstract AITranslate
Self-stratifying coating produces multicoat films by single-coat application, which offers superior performance by enhancing both the adhesion and surface properties simultaneously, suitable for many special coatings and industrial applications. Here, we have developed a well-defined multifunctional self-stratifying coating material with self-healing abilities from blending two copolymers based on fluorous/thiol/siloxane. Combinations of silyl copolymer (PMEA-co-PCMA-co-PTEPA) and fluorous copolymer (PMEA-co-PCMA-co-PHFA) offer spontaneous stratification into three layers with a gradient behavior. This transparent (>90% transmittance) coating provides a highly hydrophobic surface with good hardness (28 MPa). The polymer coating self-repairs under UV light with >80% efficiency. In addition, the healing is also conceivable by heating at 70 °C or by spraying amine due to the thiol-Michael reaction.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01102
Chinese Library Classification Number:
Citation Information:
Self-stratifying coating produces multicoat films by single-coat application, which offers superior performance by enhancing both the adhesion and surface properties simultaneously, suitable for many special coatings and industrial applications. Here, we have developed a well-defined multifunctional self-stratifying coating material with self-healing abilities from blending two copolymers based on fluorous/thiol/siloxane. Combinations of silyl copolymer (PMEA-co-PCMA-co-PTEPA) and fluorous copolymer (PMEA-co-PCMA-co-PHFA) offer spontaneous stratification into three layers with a gradient behavior. This transparent (>90% transmittance) coating provides a highly hydrophobic surface with good hardness (28 MPa). The polymer coating self-repairs under UV light with >80% efficiency. In addition, the healing is also conceivable by heating at 70 °C or by spraying amine due to the thiol-Michael reaction.
quote
| GB/T 7714-2015 | [1] Diksha Sharma, Debaprasad Mandal. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01102. |
| MLA | [1] Diksha Sharma, and Debaprasad Mandal. ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01102. |
| APA | [1] Diksha Sharma, & Debaprasad Mandal. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01102 |
| IEEE | [1] Diksha Sharma and Debaprasad Mandal, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01102. keywords: {selfstratifying;hybrid network;selfhealing;adhesion strength;coating} |