daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Constructing Cation-Coupled MoSe2/FeSe/C Heterostructures for Rapid and Efficient Sodium Ion Transport AITranslate

University of Malaya; Hebei University of Science and Technology; Hebei University of Science and Technology; Hebei University of Science and Technology; University of Malaya; Charmo University;Info-Matic Power Sdn. Bhd., Wangsa Maju; University of Malaya; Hebei University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Low electron conductivity and slow ion dynamics are the two key barriers limiting the use of transition-metal selenide (TMSe) anodes for high-power energy storage device applications. A rational structural design for TMSe can effectively promote the rapid transfer of Na+ on the surface and bulk phase. Presently, a cation-coupled MoSe2/FeSe/C heterostructure is developed by a facile two-step reaction and applied to sodium ion batteries/capacitors (SIBs/SICs). Wherein, a unique edge mixed phase (1T/2H-MoSe2) is generated under Fe induction. Additionally, the metal–organic framework-derived carbon guarantees structural stability and provides support for the rapid adsorption and transport of Na+ on the surface and bulk. Significantly, density functional theory (DFT) calculations verify that the constructed MoSe2/FeSe heterogeneous interface has a strong metallic property that can facilitate the rapid transfer of electrons and ions within the bulk phase. As a result, the prepared MoSe2/FeSe/C can deliver a high specific capacity of 597.2 mA h g–1 (after 1000 cycles) at a current density of 2 A g–1 when applied as the anode of SIBs. Impressively, 3000 cycles can be stabilized, even at a high current density of 10 A g–1. When applied to SIC anodes, a capacity retention of 80.4% can be achieved at 2 A g–1 after 8000 cycles. The strategy of combining cation-coupled induced phase transitions with heterostructure design can serve as a reference for exploring the potential of TMSe in high-power energy storage devices.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c01301

Chinese Library Classification Number:

Citation Information:

Low electron conductivity and slow ion dynamics are the two key barriers limiting the use of transition-metal selenide (TMSe) anodes for high-power energy storage device applications. A rational structural design for TMSe can effectively promote the rapid transfer of Na+ on the surface and bulk phase. Presently, a cation-coupled MoSe2/FeSe/C heterostructure is developed by a facile two-step reaction and applied to sodium ion batteries/capacitors (SIBs/SICs). Wherein, a unique edge mixed phase (1T/2H-MoSe2) is generated under Fe induction. Additionally, the metal–organic framework-derived carbon guarantees structural stability and provides support for the rapid adsorption and transport of Na+ on the surface and bulk. Significantly, density functional theory (DFT) calculations verify that the constructed MoSe2/FeSe heterogeneous interface has a strong metallic property that can facilitate the rapid transfer of electrons and ions within the bulk phase. As a result, the prepared MoSe2/FeSe/C can deliver a high specific capacity of 597.2 mA h g–1 (after 1000 cycles) at a current density of 2 A g–1 when applied as the anode of SIBs. Impressively, 3000 cycles can be stabilized, even at a high current density of 10 A g–1. When applied to SIC anodes, a capacity retention of 80.4% can be achieved at 2 A g–1 after 8000 cycles. The strategy of combining cation-coupled induced phase transitions with heterostructure design can serve as a reference for exploring the potential of TMSe in high-power energy storage devices.

quote

GB/T 7714-2015 [1] Jian Wang, Zhaojin Li, Qiujun Wang, et al. ACS Materials Letters, 2024(6). DOI:10.1021/acsmaterialslett.3c01301.
MLA [1] Jian Wang, et al., ACS Materials Letters, no. 6, 2024, https://doi.org/10.1021/acsmaterialslett.3c01301.
APA [1] Jian Wang, Zhaojin Li, Qiujun Wang, Huilan Sun, Haw Jiunn Woo, Shujahadeen B. Aziz, N. Z. Nik Husin, Ramesh T. Subramaniam, & Bo Wang. (2024). ACS Materials Letters(6). https://doi.org/10.1021/acsmaterialslett.3c01301
IEEE [1] Jian Wang, Zhaojin Li, Qiujun Wang, Huilan Sun, Haw Jiunn Woo, Shujahadeen B. Aziz, N. Z. Nik Husin, Ramesh T. Subramaniam, and Bo Wang, ACS Materials Letters, no. 6, 2024, doi: 10.1021/acsmaterialslett.3c01301.