Upper Critical Solution Temperature Type Thermoresponsive Reactive Copolymers for Enzyme Immobilization AITranslate

University of Bayreuth; University of Bayreuth; University of Bayreuth
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Functional thermoresponsive copolymers poly(N-acryloyl glycinamide-co-glycidyl methacrylate) (PNAGA-co-GMA) and poly(N-acryloyl glycinamide-co-N-(methacrylate)succinimide) (PNAGA-co-MNHS) were prepared by free-radical polymerization. With increasing functional comonomer content, the phase transition temperature increased. The functional copolymers reacted with the enzyme α-amylase by W/O emulsion to form water-soluble biohybrid nanogels. The hydrodynamic radius of biohybrid nanogels increased with temperature due to thermophilic swelling. Biohybrid nanogels of PNAGA-co-GMA and PNAGA-co-MNHS revealed a 1.2- and 1.5-fold increase of enzyme activity at 40 and 15 °C, respectively. Free α-amylase showed a 1.1-fold increase in comparison. Therefore, nanogels of these reactive thermoresponsive copolymers could be used to modulate the enzyme activity of various enzymes. As reactive polymers, they could be used as an initiation site for grafting polymerization to introduce functionality to PNAGA copolymers in further work.

KeyWords AITranslate

thermoresponsive thermosensitive nanogel phase transitions UCST enzyme immobilization hydrogel copolymer
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00448

Chinese Library Classification Number:

Citation Information:

Functional thermoresponsive copolymers poly(N-acryloyl glycinamide-co-glycidyl methacrylate) (PNAGA-co-GMA) and poly(N-acryloyl glycinamide-co-N-(methacrylate)succinimide) (PNAGA-co-MNHS) were prepared by free-radical polymerization. With increasing functional comonomer content, the phase transition temperature increased. The functional copolymers reacted with the enzyme α-amylase by W/O emulsion to form water-soluble biohybrid nanogels. The hydrodynamic radius of biohybrid nanogels increased with temperature due to thermophilic swelling. Biohybrid nanogels of PNAGA-co-GMA and PNAGA-co-MNHS revealed a 1.2- and 1.5-fold increase of enzyme activity at 40 and 15 °C, respectively. Free α-amylase showed a 1.1-fold increase in comparison. Therefore, nanogels of these reactive thermoresponsive copolymers could be used to modulate the enzyme activity of various enzymes. As reactive polymers, they could be used as an initiation site for grafting polymerization to introduce functionality to PNAGA copolymers in further work.

quote

GB/T 7714-2015 [1] Nikola Majstorović, Jens Pechtold, Seema Agarwal. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00448.
MLA [1] Nikola Majstorović, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00448.
APA [1] Nikola Majstorović, Jens Pechtold, & Seema Agarwal. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00448
IEEE [1] Nikola Majstorović, Jens Pechtold, and Seema Agarwal, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00448. keywords: {thermoresponsive;thermosensitive;nanogel;phase transitions;UCST;enzyme immobilization;hydrogel;copolymer}