Thermodynamic modelling of an Al2O3–MnO system using the ionic model AITranslate
Abstract AITranslate
The thermodynamic assessment of an Al2O3–MnO pseudo-binary system has been carried out with the use of an ionic model. The use of the electro-neutrality principles in addition to the constitutive relations, between site fractions of the species on each sub-lattice, the thermodynamics descriptions of each solid phase has been determined to make possible the solubility description. Based on the thermodynamics descriptions of each phase in addition to thermo-chemical data obtained from the literature, the Gibbs energy functions were optimized for each phase of the Al2O3–MnO system with the support of PARROT®module from ThemoCalc®package. A thermodynamic database was obtained, in agreement with the thermo-chemical data extracted from the literature, to describe the Al2O3–MnO system including the solubility description of solid phases.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2009.09.003
Chinese Library Classification Number:
Citation Information:
The thermodynamic assessment of an Al2O3–MnO pseudo-binary system has been carried out with the use of an ionic model. The use of the electro-neutrality principles in addition to the constitutive relations, between site fractions of the species on each sub-lattice, the thermodynamics descriptions of each solid phase has been determined to make possible the solubility description. Based on the thermodynamics descriptions of each phase in addition to thermo-chemical data obtained from the literature, the Gibbs energy functions were optimized for each phase of the Al2O3–MnO system with the support of PARROT®module from ThemoCalc®package. A thermodynamic database was obtained, in agreement with the thermo-chemical data extracted from the literature, to describe the Al2O3–MnO system including the solubility description of solid phases.
quote
| GB/T 7714-2015 | [1] Alexandre Bellegard Farina, Flávio Beneduce Neto. Calphad, 2009(33). DOI:10.1016/j.calphad.2009.09.003. |
| MLA | [1] Alexandre Bellegard Farina, and Flávio Beneduce Neto. Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2009.09.003. |
| APA | [1] Alexandre Bellegard Farina, & Flávio Beneduce Neto. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2009.09.003 |
| IEEE | [1] Alexandre Bellegard Farina and Flávio Beneduce Neto, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2009.09.003. |