Bifunctional MoS2 coated melamine-formaldehyde sponges for efficient oil–water separation and water-soluble dye removal AITranslate
Abstract AITranslate
Removal of pollutants from water is an important global challenge for energy conservation and environmental protection. Advanced macro-porous sorbent materials with three-dimensional wettability surfaces have been considered traditional candidates for wastewater treatment. Although the real water environment always co-exists with two pollution sources, the major functions of existing macro-porous materials are limited to either water-insoluble organics separation or water-soluble dyes removal. Bifunctional macro-porous materials for simultaneous oil–water separation and soluble elements removal are currently lacking. Here we report the novel MoS2-coated melamine-formaldehyde (MF@MoS2) sponges with different wettabilities, for example, superhydrophobicity and superhydrophilicity, exhibiting both high selectivity and excellent absorption capacities for a wide range of oils/organic solvents with different densities and water-soluble dyes. The functional MF@MoS2 sponges perform high absorption capacity for different organic solvents up to 66 and 157 times of its own weight respectively, while showing high discoloration efficiency of 98% methyl orange within 10 min. For the first time, we report these functional macro-porous materials used for simultaneous cleaning of oil and soluble pollutants in water, which extended the potential of MoS2 for environmental application. Furthermore, a continuous and simultaneous removal of insoluble oils and soluble dyes in situ from water was achieved by simply applying external pumping on the functional macro-porous MF@MoS2 sponges. Graphical abstract Download : Download high-res image (112KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.apmt.2017.09.013
Chinese Library Classification Number:
Citation Information:
Removal of pollutants from water is an important global challenge for energy conservation and environmental protection. Advanced macro-porous sorbent materials with three-dimensional wettability surfaces have been considered traditional candidates for wastewater treatment. Although the real water environment always co-exists with two pollution sources, the major functions of existing macro-porous materials are limited to either water-insoluble organics separation or water-soluble dyes removal. Bifunctional macro-porous materials for simultaneous oil–water separation and soluble elements removal are currently lacking. Here we report the novel MoS2-coated melamine-formaldehyde (MF@MoS2) sponges with different wettabilities, for example, superhydrophobicity and superhydrophilicity, exhibiting both high selectivity and excellent absorption capacities for a wide range of oils/organic solvents with different densities and water-soluble dyes. The functional MF@MoS2 sponges perform high absorption capacity for different organic solvents up to 66 and 157 times of its own weight respectively, while showing high discoloration efficiency of 98% methyl orange within 10 min. For the first time, we report these functional macro-porous materials used for simultaneous cleaning of oil and soluble pollutants in water, which extended the potential of MoS2 for environmental application. Furthermore, a continuous and simultaneous removal of insoluble oils and soluble dyes in situ from water was achieved by simply applying external pumping on the functional macro-porous MF@MoS2 sponges. Graphical abstract Download : Download high-res image (112KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Zuteng Wan, De Li, Yanli Jiao, et al. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.09.013. |
| MLA | [1] Zuteng Wan, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.09.013. |
| APA | [1] Zuteng Wan, De Li, Yanli Jiao, Xiaoping Ouyang, Lingqian Chang, & Xiufeng Wang. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.09.013 |
| IEEE | [1] Zuteng Wan, De Li, Yanli Jiao, Xiaoping Ouyang, Lingqian Chang, and Xiufeng Wang, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.09.013. |