Dynamically Cross-Linked Waterborne Polyurethanes: Transalkylation Exchange of C–N Bonds Toward High Performance and Reprocessable Thermosets AITranslate

Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology; Hefei University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thermosetting waterborne polyurethanes (WPUs) have received wide attention because of their excellent chemical resistance, mechanical properties, and low water absorption. However, their permanent network structure hinders their reprocessing applications, making it vital to prepare reprocessable thermosetting WPUs to minimize plastic pollution. Herein, for the first time, the cross-linked WPUs with excellent reprocessability were designed and synthesized by introducing covalent adaptable networks (CANs) in the form of quaternary ammonium alkyl chains. Our methodology combined CO2-triggered WPUs (CO2-triggered WPUs) with 1,6-diiodohexane. After the CO2 evaporated during film formation, the CO2-triggered WPUs left tertiary amine groups as reaction precursors, which could cross-link into a WPU CAN with 1,6-diiodohexane. All cross-linked WPUs possessed classic vitrimer performance including stress relaxation and malleability, as confirmed by stress-relaxation and hot-press tests. The results showed that cross-linked WPUs had excellent reprocessability and high mechanical properties, and the recovery ratios of the mechanical properties for the recycled samples were over 80% and the tensile strength was more than 17 MPa. More importantly, the cross-linked WPUs’ antibacterial rates of Staphylococcus aureus and Escherichia coli were 94.3 and 89.5%, respectively. This research offers a new method to synthesize high-performance WPUs via facile quaternary ammonium reversible cross-linking and demonstrates that WPU CANs have great potential as sustainable materials.

KeyWords AITranslate

CO2triggered waterborne polyurethanes covalent adaptable networks reprocessability highperformance antibacterial activity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00794

Chinese Library Classification Number:

Citation Information:

Thermosetting waterborne polyurethanes (WPUs) have received wide attention because of their excellent chemical resistance, mechanical properties, and low water absorption. However, their permanent network structure hinders their reprocessing applications, making it vital to prepare reprocessable thermosetting WPUs to minimize plastic pollution. Herein, for the first time, the cross-linked WPUs with excellent reprocessability were designed and synthesized by introducing covalent adaptable networks (CANs) in the form of quaternary ammonium alkyl chains. Our methodology combined CO2-triggered WPUs (CO2-triggered WPUs) with 1,6-diiodohexane. After the CO2 evaporated during film formation, the CO2-triggered WPUs left tertiary amine groups as reaction precursors, which could cross-link into a WPU CAN with 1,6-diiodohexane. All cross-linked WPUs possessed classic vitrimer performance including stress relaxation and malleability, as confirmed by stress-relaxation and hot-press tests. The results showed that cross-linked WPUs had excellent reprocessability and high mechanical properties, and the recovery ratios of the mechanical properties for the recycled samples were over 80% and the tensile strength was more than 17 MPa. More importantly, the cross-linked WPUs’ antibacterial rates of Staphylococcus aureus and Escherichia coli were 94.3 and 89.5%, respectively. This research offers a new method to synthesize high-performance WPUs via facile quaternary ammonium reversible cross-linking and demonstrates that WPU CANs have great potential as sustainable materials.

quote

GB/T 7714-2015 [1] Zhaofei Wang, Xuemin Zhang, Wansheng Yao, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00794.
MLA [1] Zhaofei Wang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00794.
APA [1] Zhaofei Wang, Xuemin Zhang, Wansheng Yao, Yong Dong, Baiyao Zhang, Xiaoyu Dong, Huagao Fang, Guobing Zhang, & Yunsheng Ding. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00794
IEEE [1] Zhaofei Wang, Xuemin Zhang, Wansheng Yao, Yong Dong, Baiyao Zhang, Xiaoyu Dong, Huagao Fang, Guobing Zhang, and Yunsheng Ding, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00794. keywords: {CO2triggered waterborne polyurethanes;covalent adaptable networks;reprocessability;highperformance;antibacterial activity}