Photocurable Hybrid Materials with High Magnetodielectric Coupling AITranslate

BCMaterials, Basque Center for Materials; Universidade do Minho; Universidade do Minho;Taras Shevchenko National University of Kyiv;Centre for Cooperative Research on Alternative Energies (CIC energiGUNE), Basque Research and Technology Alliance (BRTA);BCMaterials, Basque Center for Materials;BCMaterials, Basque Center for Materials;Department of Applied Science and Technology (DISAT), Politecnico di Torino; Universidade do Minho
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Magnetodielectric materials are highly interesting in the scope of Internet of Things (IoT)-related devices such as antennas, sensors, and actuators, as they allow the magnetic control of the dielectric response. Among the different possible methods for their development, the combination of photocurable polymers and magnetic nanoparticles allows more sustainable processes with high production velocities, room processing temperature, and the capability to fabricate a large variety of specific shapes with high resolution. In this context, photocurable magnetic hybrid materials based on polyurethane acrylate (PUA) and on different magnetic micro- and nanoparticles, including cobalt ferrite oxide (CFO), magnetite (Fe3O4), and a neodymium iron boron alloy (NdFeB), have been developed. The influence of filler type and content on the photopolymerization process, sample morphology, physicochemical properties, electrical conductivity, and magnetic properties has been investigated. Filler dispersion has also been studied by neutron scattering techniques, enabling the determination of the organization of the filler aggregates, which plays an essential role in the overall characteristics of the composites. Materials with maximum magnetodielectric coefficients (MD %) as large as 28% have been obtained for the sample with 6% NdFeB filler content, making these magnetic composites of paramount interest for the fabrication of magnetodielectric devices in the context of the digital transition.

KeyWords AITranslate

magnetodielectric effect UV curable nanocomposites magnetic nanoparticles neutron scattering dielectric properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01566

Chinese Library Classification Number:

Citation Information:

Magnetodielectric materials are highly interesting in the scope of Internet of Things (IoT)-related devices such as antennas, sensors, and actuators, as they allow the magnetic control of the dielectric response. Among the different possible methods for their development, the combination of photocurable polymers and magnetic nanoparticles allows more sustainable processes with high production velocities, room processing temperature, and the capability to fabricate a large variety of specific shapes with high resolution. In this context, photocurable magnetic hybrid materials based on polyurethane acrylate (PUA) and on different magnetic micro- and nanoparticles, including cobalt ferrite oxide (CFO), magnetite (Fe3O4), and a neodymium iron boron alloy (NdFeB), have been developed. The influence of filler type and content on the photopolymerization process, sample morphology, physicochemical properties, electrical conductivity, and magnetic properties has been investigated. Filler dispersion has also been studied by neutron scattering techniques, enabling the determination of the organization of the filler aggregates, which plays an essential role in the overall characteristics of the composites. Materials with maximum magnetodielectric coefficients (MD %) as large as 28% have been obtained for the sample with 6% NdFeB filler content, making these magnetic composites of paramount interest for the fabrication of magnetodielectric devices in the context of the digital transition.

quote

GB/T 7714-2015 [1] Cristian MendesFelipe, Rui Carvalho, Pedro Martins, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01566.
MLA [1] Cristian MendesFelipe, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01566.
APA [1] Cristian MendesFelipe, Rui Carvalho, Pedro Martins, Oleksandr Igorovych Ivankov, Ivan Bobrikov, Viktor Petrenko, Jose Maria Porro, Marco Sangermano, & Senentxu LancerosMendez. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01566
IEEE [1] Cristian MendesFelipe, Rui Carvalho, Pedro Martins, Oleksandr Igorovych Ivankov, Ivan Bobrikov, Viktor Petrenko, Jose Maria Porro, Marco Sangermano, and Senentxu LancerosMendez, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01566. keywords: {magnetodielectric effect;UV curable nanocomposites;magnetic nanoparticles;neutron scattering;dielectric properties}