daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Two-Factor Phase Separations in Mixed-Halide Quasi-2D Perovskite LEDs: Dimensionality and Halide Segregations AITranslate

Purdue University; Purdue University; Argonne National Laboratory; Purdue University; Purdue University; Lawrence Berkeley National Laboratory; Purdue University; Purdue University; Argonne National Laboratory; Lawrence Berkeley National Laboratory; Purdue University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Quasi-2D halide perovskites have attracted much interest as a promising material for light-emitting diodes (LEDs) due to their tunability in quantum confinement and halide alloy formation to modulate the energy bandgap and emission color. However, two-factor phase separations with respect to heterogeneous quantum-well thicknesses and halide segregation are still crucial issues in quasi-2D perovskite LEDs, leading to low external quantum efficiencies (EQEs) and color shifts. Herein, we compare quasi-2D perovskite films using different cations to unveil the key contributions from the chemical design of organic cations. While mixing halide ions in conventional quasi-2D perovskite films induces micrometer-scale heterogeneity, new extended and twisted conjugated cations suppress the two-factor phase separations, leading to high EQEs of over 25% and controllable emission wavelengths across red and near-infrared regions. The fundamental insights in this work will provide guidance for advancing materials design and device performance in the future.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01009

Chinese Library Classification Number:

Citation Information:

Quasi-2D halide perovskites have attracted much interest as a promising material for light-emitting diodes (LEDs) due to their tunability in quantum confinement and halide alloy formation to modulate the energy bandgap and emission color. However, two-factor phase separations with respect to heterogeneous quantum-well thicknesses and halide segregation are still crucial issues in quasi-2D perovskite LEDs, leading to low external quantum efficiencies (EQEs) and color shifts. Herein, we compare quasi-2D perovskite films using different cations to unveil the key contributions from the chemical design of organic cations. While mixing halide ions in conventional quasi-2D perovskite films induces micrometer-scale heterogeneity, new extended and twisted conjugated cations suppress the two-factor phase separations, leading to high EQEs of over 25% and controllable emission wavelengths across red and near-infrared regions. The fundamental insights in this work will provide guidance for advancing materials design and device performance in the future.

quote

GB/T 7714-2015 [1] Seok Joo Yang, Kang Wang, Yanqi Luo, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01009.
MLA [1] Seok Joo Yang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01009.
APA [1] Seok Joo Yang, Kang Wang, Yanqi Luo, Jee Yung Park, Hanjun Yang, Aidan H. Coffey, Ke Ma, Jiaonan Sun, Sarah Wieghold, Chenhui Zhu, & Letian Dou. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01009
IEEE [1] Seok Joo Yang, Kang Wang, Yanqi Luo, Jee Yung Park, Hanjun Yang, Aidan H. Coffey, Ke Ma, Jiaonan Sun, Sarah Wieghold, Chenhui Zhu, and Letian Dou, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01009.