Amphiphilic TEMPO-Functionalized Block Copolymers: Synthesis, Self-Assembly and Redox-Responsive Disassembly Behavior, and Potential Application in Triggered Drug Delivery AITranslate

Zhejiang University of Technology; Zhejiang University of Technology; Zhejiang University of Technology; Hebei University; Zhejiang University of Technology; Concordia University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A novel range of amphiphilic redox-responsive 2,2,6,6-tetramethylpiperidine-1-oxyl (TEMPO)-functionalized diblock copolymers poly(ethylene glycol)-b-poly(2,2,6,6-tetramethylpiperidine-1-oxyl-4-yl methacrylate-co-N-isopropylacrylamide [PEG-b-P(TMA-co-NIPAM)] have been synthesized in this work via reversible addition–fragmentation chain transfer (RAFT) polymerization followed with functionality transformation. With the possession of the hydrophilic PEG block and the hydrophobic TEMPO-containing block, these amphiphilic diblock polymers can conveniently self-assemble to form stable uniformly sized radical-containing nanoparticles (RNPs), which can thus act as nanovessels to carry drugs. More interestingly, the self-assembled RNPs exhibit the unique reduction-responsive disassembly upon addition of vitamin C (VC) as a representative reducing agent due to the drastic drop in the surface hydrophobicity following reduction of the TEMPO units. In the proof-of-concept experiments, the VC-triggered release of the encapsulated R6G dye as the model payload from the RNPs at controllable rates has been successfully demonstrated. Meanwhile, the cytotoxicity study with CCK-8 assay confirms the TEMPO-containing block copolymers and their reduced ones are nontoxic at a concentration up to 500 μg mL–1. This series of amphiphilic diblock copolymers is thus highly promising for potential application in triggered drug delivery.

KeyWords AITranslate

amphiphilic copolymers redoxresponsive behavior TEMPO nanovessels triggered drug delivery
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00293

Chinese Library Classification Number:

Citation Information:

A novel range of amphiphilic redox-responsive 2,2,6,6-tetramethylpiperidine-1-oxyl (TEMPO)-functionalized diblock copolymers poly(ethylene glycol)-b-poly(2,2,6,6-tetramethylpiperidine-1-oxyl-4-yl methacrylate-co-N-isopropylacrylamide [PEG-b-P(TMA-co-NIPAM)] have been synthesized in this work via reversible addition–fragmentation chain transfer (RAFT) polymerization followed with functionality transformation. With the possession of the hydrophilic PEG block and the hydrophobic TEMPO-containing block, these amphiphilic diblock polymers can conveniently self-assemble to form stable uniformly sized radical-containing nanoparticles (RNPs), which can thus act as nanovessels to carry drugs. More interestingly, the self-assembled RNPs exhibit the unique reduction-responsive disassembly upon addition of vitamin C (VC) as a representative reducing agent due to the drastic drop in the surface hydrophobicity following reduction of the TEMPO units. In the proof-of-concept experiments, the VC-triggered release of the encapsulated R6G dye as the model payload from the RNPs at controllable rates has been successfully demonstrated. Meanwhile, the cytotoxicity study with CCK-8 assay confirms the TEMPO-containing block copolymers and their reduced ones are nontoxic at a concentration up to 500 μg mL–1. This series of amphiphilic diblock copolymers is thus highly promising for potential application in triggered drug delivery.

quote

GB/T 7714-2015 [1] Xianbo Shen, Shixiong Cao, Qi Zhang, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00293.
MLA [1] Xianbo Shen, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00293.
APA [1] Xianbo Shen, Shixiong Cao, Qi Zhang, Jinchao Zhang, Jianli Wang, & Zhibin Ye. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00293
IEEE [1] Xianbo Shen, Shixiong Cao, Qi Zhang, Jinchao Zhang, Jianli Wang, and Zhibin Ye, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00293. keywords: {amphiphilic copolymers;redoxresponsive behavior;TEMPO;nanovessels;triggered drug delivery}