Enhanced Stability and Efficiency for Photoelectrochemical Iodide Oxidation by Methyl Termination and Electrochemical Pt Deposition on n-Type Si Microwire Arrays AITranslate
Abstract AITranslate
Arrays of Si microwires doped n-type (n-Si) and surface-functionalized with methyl groups have been used, with or without deposition of Pt electrocatalysts, to photoelectrochemically oxidize I–(aq) to I3–(aq) in 7.6 M HI(aq). Under conditions of iodide oxidation, methyl-terminated n-Si microwire arrays exhibited stable short-circuit photocurrents over a time scale of days, albeit with low energy-conversion efficiencies. In contrast, electrochemical deposition of Pt onto methyl-terminated n-Si microwire arrays consistently yielded energy-conversion efficiencies of ∼2% for iodide oxidation, with an open-circuit photovoltage of ∼400 mV and a short-circuit photocurrent density of ∼10 mA cm–2 under 100 mW cm–2 of simulated air mass 1.5G solar illumination. Platinized electrodes were stable for >200 h of continuous operation, with no discernible loss of Si or Pt. Pt deposited using electron-beam evaporation also resulted in stable photoanodic operation of the methyl-terminated n-Si microwire arrays but yielded substantially lower photovoltages than when Pt was deposited electrochemically.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b01529
Chinese Library Classification Number:
Citation Information:
Arrays of Si microwires doped n-type (n-Si) and surface-functionalized with methyl groups have been used, with or without deposition of Pt electrocatalysts, to photoelectrochemically oxidize I–(aq) to I3–(aq) in 7.6 M HI(aq). Under conditions of iodide oxidation, methyl-terminated n-Si microwire arrays exhibited stable short-circuit photocurrents over a time scale of days, albeit with low energy-conversion efficiencies. In contrast, electrochemical deposition of Pt onto methyl-terminated n-Si microwire arrays consistently yielded energy-conversion efficiencies of ∼2% for iodide oxidation, with an open-circuit photovoltage of ∼400 mV and a short-circuit photocurrent density of ∼10 mA cm–2 under 100 mW cm–2 of simulated air mass 1.5G solar illumination. Platinized electrodes were stable for >200 h of continuous operation, with no discernible loss of Si or Pt. Pt deposited using electron-beam evaporation also resulted in stable photoanodic operation of the methyl-terminated n-Si microwire arrays but yielded substantially lower photovoltages than when Pt was deposited electrochemically.
quote
| GB/T 7714-2015 | [1] Shane Ardo, Elizabeth A. Santori, Hal S. Emmer, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01529. |
| MLA | [1] Shane Ardo, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01529. |
| APA | [1] Shane Ardo, Elizabeth A. Santori, Hal S. Emmer, Ronald L. Grimm, Matthew J. Bierman, Bruce S. Brunschwig, Harry A. Atwater, & Nathan S. Lewis. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01529 |