Double-Helicene-Based Hole-Transporter for Perovskite Solar Cells with 22% Efficiency and Operation Durability AITranslate

Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University; Zhejiang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Amelioration of the mobility and, in particular, the thermal stability of a hole-transporting molecular semiconductor is a practicable strategy to attain the enhancement of both power conversion efficiency (PCE) and operational durability of perovskite solar cells (PSCs). Here a cost-effective double-[4]helicene-based molecular semiconductor (DBC-OMeDPA) is synthesized for a solution-deposited thin film, exhibiting an improved hole mobility in comparison with state-of-the-art spiro-OMeTAD control. X-ray crystallographic analysis and theoretical calculation reveal the three-dimensional molecular stacking and multidirectional hole-transporting property of DBC-OMeDPA, clarifying the microscopic mechanism of the hole-transport process. A better PCE of 22% at the AM 1.5G conditions is achieved for PSCs with DBC-OMeDPA as the hole-transporter. Moreover, PSCs using DBC-OMeDPA characteristic of an elevated intrinsic glass transition temperature of 154 °C maintain a stable PCE output for hundreds of hours at 60 °C under equivalent full sunglight soaking.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01949

Chinese Library Classification Number:

Citation Information:

Amelioration of the mobility and, in particular, the thermal stability of a hole-transporting molecular semiconductor is a practicable strategy to attain the enhancement of both power conversion efficiency (PCE) and operational durability of perovskite solar cells (PSCs). Here a cost-effective double-[4]helicene-based molecular semiconductor (DBC-OMeDPA) is synthesized for a solution-deposited thin film, exhibiting an improved hole mobility in comparison with state-of-the-art spiro-OMeTAD control. X-ray crystallographic analysis and theoretical calculation reveal the three-dimensional molecular stacking and multidirectional hole-transporting property of DBC-OMeDPA, clarifying the microscopic mechanism of the hole-transport process. A better PCE of 22% at the AM 1.5G conditions is achieved for PSCs with DBC-OMeDPA as the hole-transporter. Moreover, PSCs using DBC-OMeDPA characteristic of an elevated intrinsic glass transition temperature of 154 °C maintain a stable PCE output for hundreds of hours at 60 °C under equivalent full sunglight soaking.

quote

GB/T 7714-2015 [1] Ming Ren, Jianan Wang, Xinrui Xie, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01949.
MLA [1] Ming Ren, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01949.
APA [1] Ming Ren, Jianan Wang, Xinrui Xie, Jing Zhang, & Peng Wang. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01949
IEEE [1] Ming Ren, Jianan Wang, Xinrui Xie, Jing Zhang, and Peng Wang, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01949.