This review discusses recent advances in materials engineering to control thermal conductivity. We begin by presenting theories of heat conduction for general material classes, focusing on common approximations and trends. Next, we discuss characterization techniques for measuring thermal conductivity and the underlying transport properties. Advanced materials at the frontiers of thermal transport, such as rattlers, complex unit cells, nanowires, and nanocomposites, are treated in depth using experimental data and theoretical predictions. The review closes by highlighting several promising areas for further development.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1146/annurev-matsci-070511-155040
Chinese Library Classification Number:
Citation Information:
This review discusses recent advances in materials engineering to control thermal conductivity. We begin by presenting theories of heat conduction for general material classes, focusing on common approximations and trends. Next, we discuss characterization techniques for measuring thermal conductivity and the underlying transport properties. Advanced materials at the frontiers of thermal transport, such as rattlers, complex unit cells, nanowires, and nanocomposites, are treated in depth using experimental data and theoretical predictions. The review closes by highlighting several promising areas for further development.
quote
| GB/T 7714-2015 | [1] Eric S. Toberer, Lauryn L. Baranowski, Chris Dames. Annual Review of Materials Research, 2012(42). DOI:10.1146/annurev-matsci-070511-155040. |
| MLA | [1] Eric S. Toberer, et al., Annual Review of Materials Research, no. 42, 2012, https://doi.org/10.1146/annurev-matsci-070511-155040. |
| APA | [1] Eric S. Toberer, Lauryn L. Baranowski, & Chris Dames. (2012). Annual Review of Materials Research(42). https://doi.org/10.1146/annurev-matsci-070511-155040 |
| IEEE | [1] Eric S. Toberer, Lauryn L. Baranowski, and Chris Dames, Annual Review of Materials Research, no. 42, 2012, doi: 10.1146/annurev-matsci-070511-155040. keywords: {nanostructures;nanowires;transport;thermoelectrics;thermal barrier coatings;thin films} |