daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hysteresis-Free Lead-Free Double-Perovskite Solar Cells by Interface Engineering AITranslate

University of Duisburg-Essen; Institute of Chemical Sciences and Engineering; Institute of Chemical Sciences and Engineering; Institute of Chemical Sciences and Engineering; University of Duisburg-Essen; University of Duisburg-Essen; Institute of Chemical Sciences and Engineering; University of Duisburg-Essen; Institute of Chemical Sciences and Engineering
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hybrid perovskite solar cells have been creating considerable excitement in the photovoltaic community. However, they still rely on toxic elements, which impose severe limits on their commercialization. Lead-free double hybrid perovskites in the form of Cs2AgBiBr6 have been shown to be a promising nontoxic and highly stable alternative. Nevertheless, device development is still in its infancy, and performance is affected by severe hysteresis. Here we realize for the first time hysteresis-free mesoporous double-perovskite solar cells with no s-shape in the device characteristic and increased device open-circuit voltage. This has been realized by fine-tuning the material deposition parameters, enabling the growth of a highly uniform and compact Cs2AgBiBr6, and by engineering the device interfaces by screening different molecular and polymeric hole-transporting materials. Our work represents a crucial step forward in lead-free double perovskites with significant potential for closing the gap for their market uptake.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00871

Chinese Library Classification Number:

Citation Information:

Hybrid perovskite solar cells have been creating considerable excitement in the photovoltaic community. However, they still rely on toxic elements, which impose severe limits on their commercialization. Lead-free double hybrid perovskites in the form of Cs2AgBiBr6 have been shown to be a promising nontoxic and highly stable alternative. Nevertheless, device development is still in its infancy, and performance is affected by severe hysteresis. Here we realize for the first time hysteresis-free mesoporous double-perovskite solar cells with no s-shape in the device characteristic and increased device open-circuit voltage. This has been realized by fine-tuning the material deposition parameters, enabling the growth of a highly uniform and compact Cs2AgBiBr6, and by engineering the device interfaces by screening different molecular and polymeric hole-transporting materials. Our work represents a crucial step forward in lead-free double perovskites with significant potential for closing the gap for their market uptake.

quote

GB/T 7714-2015 [1] Martina Pantaler, Kyung Taek Cho, Valentin I. E. Queloz, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00871.
MLA [1] Martina Pantaler, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00871.
APA [1] Martina Pantaler, Kyung Taek Cho, Valentin I. E. Queloz, Inés García Benito, Christian Fettkenhauer, Irina Anusca, Mohammad Khaja Nazeeruddin, Doru C. Lupascu, & Giulia Grancini. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00871
IEEE [1] Martina Pantaler, Kyung Taek Cho, Valentin I. E. Queloz, Inés García Benito, Christian Fettkenhauer, Irina Anusca, Mohammad Khaja Nazeeruddin, Doru C. Lupascu, and Giulia Grancini, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00871.