Electrochemical Reduction of Carbon Dioxide on Nitrogen-Doped Carbons: Insights from Isotopic Labeling Studies AITranslate

University of Szeged; University of Szeged
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Isotopic labeling experiments were performed to better understand the electrochemical reduction of carbon dioxide on nitrogen-doped porous carbon electrodes. By using nonequilibrated solutions of selectively labeled initial carbon sources (i.e., 13CO2 and H13CO3–), bicarbonate anion was identified as the predominant source of the carbon monoxide reduction product.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00212

Chinese Library Classification Number:

Citation Information:

Isotopic labeling experiments were performed to better understand the electrochemical reduction of carbon dioxide on nitrogen-doped porous carbon electrodes. By using nonequilibrated solutions of selectively labeled initial carbon sources (i.e., 13CO2 and H13CO3–), bicarbonate anion was identified as the predominant source of the carbon monoxide reduction product.

quote

GB/T 7714-2015 [1] Dorottya Hursán, Csaba Janáky. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00212.
MLA [1] Dorottya Hursán, and Csaba Janáky. ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00212.
APA [1] Dorottya Hursán, & Csaba Janáky. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00212
IEEE [1] Dorottya Hursán and Csaba Janáky, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00212.