Regulating the Zn deposition orientation is an efficient way to suppress Zn dendrites and stabilize Zn anodes in aqueous Zn ion batteries (ZIBs). Few studies have been conducted to control Zn(002) deposition by altering the Zn2+ solvation structure with a cosolvent. Herein, the bifunctional high-polarity cosolvent hexamethylphosphoramide (HMPA) is proposed in an aqueous electrolyte. It not only suppresses the H2 evolution reaction via the reshaped Zn2+ solvation structure with decreased H2O activity but also induces Zn(002) deposition with a hexagonal-close-packed morphology due to the strong absorption ability of HMPA to Zn(002). With the optimized electrolyte, Zn dendrites and the HER are suppressed and an ultralong cycle life of 1500 cycles with 99.6% Coulombic efficiency is achieved in Zn||Cu cells. Zn||NH4V5O10 and Zn||polyaniline full cells exhibit improved cycling performances compared to that of the bare electrolyte. Our finding provides a feasible and promising way to stabilize Zn anodes and promote the commercial application of ZIBs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02359
Chinese Library Classification Number:
Citation Information:
Regulating the Zn deposition orientation is an efficient way to suppress Zn dendrites and stabilize Zn anodes in aqueous Zn ion batteries (ZIBs). Few studies have been conducted to control Zn(002) deposition by altering the Zn2+ solvation structure with a cosolvent. Herein, the bifunctional high-polarity cosolvent hexamethylphosphoramide (HMPA) is proposed in an aqueous electrolyte. It not only suppresses the H2 evolution reaction via the reshaped Zn2+ solvation structure with decreased H2O activity but also induces Zn(002) deposition with a hexagonal-close-packed morphology due to the strong absorption ability of HMPA to Zn(002). With the optimized electrolyte, Zn dendrites and the HER are suppressed and an ultralong cycle life of 1500 cycles with 99.6% Coulombic efficiency is achieved in Zn||Cu cells. Zn||NH4V5O10 and Zn||polyaniline full cells exhibit improved cycling performances compared to that of the bare electrolyte. Our finding provides a feasible and promising way to stabilize Zn anodes and promote the commercial application of ZIBs.
quote
| GB/T 7714-2015 | [1] Zhimei Huang, Zezhuo Li, Yueda Wang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02359. |
| MLA | [1] Zhimei Huang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02359. |
| APA | [1] Zhimei Huang, Zezhuo Li, Yueda Wang, Jianlong Cong, Xiaolong Wu, Xiaohui Song, Yongxin Ma, Hongfa Xiang, & Yunhui Huang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02359 |
| IEEE | [1] Zhimei Huang, Zezhuo Li, Yueda Wang, Jianlong Cong, Xiaolong Wu, Xiaohui Song, Yongxin Ma, Hongfa Xiang, and Yunhui Huang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02359. |