Although current high-energy-density lithium-ion batteries (LIBs) have taken over the commercial rechargeable battery market, increasing concerns about limited lithium resources, high cost, and insecurity of organic electrolyte scale-up limit their further development. Rechargeable aqueous zinc-ion batteries (ZIBs), an alternative battery chemistry, have paved the way not only for realizing environmentally benign and safe energy storage devices but also for reducing the manufacturing costs of next-generation batteries. This Review underscores recent advances in aqueous ZIBs; these include the design of a highly reversible Zn anode, optimization of the electrolyte, and a wide range of cathode materials and their energy storage mechanisms. We also present recent advanced techniques that aim at overcoming the current issues in aqueous ZIB systems. This Review on the future perspectives and research directions will provide a guide for future aqueous ZIB study.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b01426
Chinese Library Classification Number:
Citation Information:
Although current high-energy-density lithium-ion batteries (LIBs) have taken over the commercial rechargeable battery market, increasing concerns about limited lithium resources, high cost, and insecurity of organic electrolyte scale-up limit their further development. Rechargeable aqueous zinc-ion batteries (ZIBs), an alternative battery chemistry, have paved the way not only for realizing environmentally benign and safe energy storage devices but also for reducing the manufacturing costs of next-generation batteries. This Review underscores recent advances in aqueous ZIBs; these include the design of a highly reversible Zn anode, optimization of the electrolyte, and a wide range of cathode materials and their energy storage mechanisms. We also present recent advanced techniques that aim at overcoming the current issues in aqueous ZIB systems. This Review on the future perspectives and research directions will provide a guide for future aqueous ZIB study.
quote
| GB/T 7714-2015 | [1] Guozhao Fang, Jiang Zhou, Anqiang Pan, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01426. |
| MLA | [1] Guozhao Fang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01426. |
| APA | [1] Guozhao Fang, Jiang Zhou, Anqiang Pan, & Shuquan Liang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01426 |
| IEEE | [1] Guozhao Fang, Jiang Zhou, Anqiang Pan, and Shuquan Liang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01426. |