Desolvation and decomposition of metal (Mn, Co and Ni)–ethylene carbonate complexes: Relevance to battery performance AITranslate
Abstract AITranslate
Highlights • Dissolved metal ions in battery electrolyte deteriorate the battery performance. • Mn2+ is the most easily desolvated (Mn2+ > Co2+ > Ni2+) on the anode surface. • Mn more readily causes a cathodic decomposition of solvent (Mn > Co ∼ Ni). Dissolved metal ions (Mn2+, Co2+, and Ni2+) present in the electrolyte are known to deteriorate the performance of the lithium-ion batteries (LIBs). In this study, ethylene carbonate (EC)-solvated M2+ and M (where M = Mn, Co, and Ni) species are examined by first-principles calculations in order to understand the detrimental impact of metal ions on LIB performance. Our calculations indicate that (1) the Mn2+ ion is the most easily desolvated (Mn2+ > Co2+ > Ni2+) and deposited at the anode surface; and (2) the Mn element more readily causes a cathodic decomposition of EC via metal-to-solvent electron transfer (Mn > Co ∼ Ni). Graphical abstract Download : Download high-res image (122KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2013.09.017
Chinese Library Classification Number:
Citation Information:
Highlights • Dissolved metal ions in battery electrolyte deteriorate the battery performance. • Mn2+ is the most easily desolvated (Mn2+ > Co2+ > Ni2+) on the anode surface. • Mn more readily causes a cathodic decomposition of solvent (Mn > Co ∼ Ni). Dissolved metal ions (Mn2+, Co2+, and Ni2+) present in the electrolyte are known to deteriorate the performance of the lithium-ion batteries (LIBs). In this study, ethylene carbonate (EC)-solvated M2+ and M (where M = Mn, Co, and Ni) species are examined by first-principles calculations in order to understand the detrimental impact of metal ions on LIB performance. Our calculations indicate that (1) the Mn2+ ion is the most easily desolvated (Mn2+ > Co2+ > Ni2+) and deposited at the anode surface; and (2) the Mn element more readily causes a cathodic decomposition of EC via metal-to-solvent electron transfer (Mn > Co ∼ Ni). Graphical abstract Download : Download high-res image (122KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] YoungKyu Han, Keonjoon Lee, Sunwoo Kang, et al. Computational Materials Science, 2014(81). DOI:10.1016/j.commatsci.2013.09.017. |
| MLA | [1] YoungKyu Han, et al., Computational Materials Science, no. 81, 2014, https://doi.org/10.1016/j.commatsci.2013.09.017. |
| APA | [1] YoungKyu Han, Keonjoon Lee, Sunwoo Kang, Yun Suk Huh, & Hochun Lee. (2014). Computational Materials Science(81). https://doi.org/10.1016/j.commatsci.2013.09.017 |
| IEEE | [1] YoungKyu Han, Keonjoon Lee, Sunwoo Kang, Yun Suk Huh, and Hochun Lee, Computational Materials Science, no. 81, 2014, doi: 10.1016/j.commatsci.2013.09.017. |