Durable Superhydrophobic Poly(vinylidene fluoride) (PVDF)-Based Nanofibrous Membranes for Reusable Air Filters AITranslate
Abstract AITranslate
We present a durable superhydrophobic poly(vinylidene fluoride) (PVDF)-based nanofibrous membrane to achieve high-performance air filters with reusability. We demonstrate that the additional assembly of silica nanoparticles on an electrospun PVDF nanofibrous membrane and subsequent low-surface-energy treatment enables nonwetting of various probing liquids and the membrane to exhibit a low roll-off angle (∼15°) even for 1 μL of water and artificial saliva droplets. This allows fine dust particles adsorbed on the modified PVDF membrane to be easily removed by washing and suppresses the adhesion of bacterial suspension. Moreover, the modified membrane is compatible with the ethanol sterilization procedure as the membrane exhibits no noticeable alteration in the structure and surface wettability upon spraying or dipping in 75% ethanol solution. Furthermore, by applying these modified PVDF nanofibrous membranes as a skin layer on top of an unmodified analogue, we demonstrate that air filters with high filtration performance, mechanical strength, and reusability can be prepared.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01314
Chinese Library Classification Number:
Citation Information:
We present a durable superhydrophobic poly(vinylidene fluoride) (PVDF)-based nanofibrous membrane to achieve high-performance air filters with reusability. We demonstrate that the additional assembly of silica nanoparticles on an electrospun PVDF nanofibrous membrane and subsequent low-surface-energy treatment enables nonwetting of various probing liquids and the membrane to exhibit a low roll-off angle (∼15°) even for 1 μL of water and artificial saliva droplets. This allows fine dust particles adsorbed on the modified PVDF membrane to be easily removed by washing and suppresses the adhesion of bacterial suspension. Moreover, the modified membrane is compatible with the ethanol sterilization procedure as the membrane exhibits no noticeable alteration in the structure and surface wettability upon spraying or dipping in 75% ethanol solution. Furthermore, by applying these modified PVDF nanofibrous membranes as a skin layer on top of an unmodified analogue, we demonstrate that air filters with high filtration performance, mechanical strength, and reusability can be prepared.
quote
| GB/T 7714-2015 | [1] Hyeongjeong Kim, Sukyoung Lee, Ye Rim Shin, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01314. |
| MLA | [1] Hyeongjeong Kim, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01314. |
| APA | [1] Hyeongjeong Kim, Sukyoung Lee, Ye Rim Shin, YunNam Choi, Jongsun Yoon, Min Ryu, Jeong Wook Lee, & Hyomin Lee. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01314 |
| IEEE | [1] Hyeongjeong Kim, Sukyoung Lee, Ye Rim Shin, YunNam Choi, Jongsun Yoon, Min Ryu, Jeong Wook Lee, and Hyomin Lee, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01314. keywords: {nanofiber;filter;reusable;superhydrophobic;PVDF} |