Enabling Lattice Oxygen Participation in a Triple Perovskite Oxide Electrocatalyst for the Oxygen Evolution Reaction AITranslate

Jeonbuk National University; Jeonbuk National University; Jeonbuk National University; Jeonbuk National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Perovskite oxides are considered to be attractive catalysts for the electrocatalysis of water in an alkaline electrolyte. However, they suffer from low catalytic efficacy and stability that need to be further improved. Here we present a triple perovskite, Sr3NiFeMoO9−δ (SNFM), as a promising oxygen evolution electrocatalyst with high durability that outperforms double and single perovskites. The high performance of the triple perovskite SNFM could be correlated to the high lattice oxygen participation observed via pH-dependent oxygen evolution reaction (OER) activity on the reversible hydrogen electrode scale. Through the strong participation of the oxide lattice during O2 evolution in SNFM, the kinetic limitation can be eliminated, as it occurs during the conventional adsorbate evolution mechanism. In addition to lattice oxygen participation, SNFM exhibits a low charge transfer resistance at different potentials, studied through operando electrochemical impedance spectroscopy, and a high oxygen diffusion rate that is related to its oxygen vacancy defects.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02617

Chinese Library Classification Number:

Citation Information:

Perovskite oxides are considered to be attractive catalysts for the electrocatalysis of water in an alkaline electrolyte. However, they suffer from low catalytic efficacy and stability that need to be further improved. Here we present a triple perovskite, Sr3NiFeMoO9−δ (SNFM), as a promising oxygen evolution electrocatalyst with high durability that outperforms double and single perovskites. The high performance of the triple perovskite SNFM could be correlated to the high lattice oxygen participation observed via pH-dependent oxygen evolution reaction (OER) activity on the reversible hydrogen electrode scale. Through the strong participation of the oxide lattice during O2 evolution in SNFM, the kinetic limitation can be eliminated, as it occurs during the conventional adsorbate evolution mechanism. In addition to lattice oxygen participation, SNFM exhibits a low charge transfer resistance at different potentials, studied through operando electrochemical impedance spectroscopy, and a high oxygen diffusion rate that is related to its oxygen vacancy defects.

quote

GB/T 7714-2015 [1] Anuj Kumar Tomar, Uday Narayan Pan, Nam Hoon Kim, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02617.
MLA [1] Anuj Kumar Tomar, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02617.