daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Recent progress on V2O5 based electroactive materials: Synthesis, properties, and supercapacitor application AITranslate

Hawassa University; King Faisal University; University of Nigeria Nsukka; King Faisal University; University of Nigeria; University of Nigeria Nsukka; University of South Africa
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The concerns of sustainable energy rely on highly efficient renewable energy sources and effective storage devices. Supercapacitor is practically reliable energy storage devices with rapid charging rate, high power density, simple setup, and good stability. Electrode materials have significant impacts on the performance of supercapacitors. Therefore, finding high-performing electroactive material is a critical concern of the area. Herein, the recent progress of vanadium pentoxide-based electroactive materials for supercapacitor application has been reviewed. Vanadium pentoxide is a potential electroactive material for supercapacitor due to its mixed oxidation states, eco-friendliness, low cost, high capacitance, and high energy density. But, poor conductivity and low cyclic stability are major drawbacks of the oxide which affect its electrochemical properties. This review points out different strategies of mitigating such limitations. Finally, future perspectives on V2O5-based electroactive materials for supercapacitor application have been highlighted. Graphical abstract Download : Download high-res image (277KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.coelec.2023.101239

Chinese Library Classification Number:

Citation Information:

The concerns of sustainable energy rely on highly efficient renewable energy sources and effective storage devices. Supercapacitor is practically reliable energy storage devices with rapid charging rate, high power density, simple setup, and good stability. Electrode materials have significant impacts on the performance of supercapacitors. Therefore, finding high-performing electroactive material is a critical concern of the area. Herein, the recent progress of vanadium pentoxide-based electroactive materials for supercapacitor application has been reviewed. Vanadium pentoxide is a potential electroactive material for supercapacitor due to its mixed oxidation states, eco-friendliness, low cost, high capacitance, and high energy density. But, poor conductivity and low cyclic stability are major drawbacks of the oxide which affect its electrochemical properties. This review points out different strategies of mitigating such limitations. Finally, future perspectives on V2O5-based electroactive materials for supercapacitor application have been highlighted. Graphical abstract Download : Download high-res image (277KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Abdudin G. Temam, Adil Alshoaibi, Seyoum A. Getaneh, et al. Current Opinion in Electrochemistry, 2023(38). DOI:10.1016/j.coelec.2023.101239.
MLA [1] Abdudin G. Temam, et al., Current Opinion in Electrochemistry, no. 38, 2023, https://doi.org/10.1016/j.coelec.2023.101239.