Room-Temperature Lateral Spin Valve in Graphene/Fe3GaTe2 van der Waals Heterostructures AITranslate

Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Tezpur University (Central University); Nanyang Technological University; National University of Singapore
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The remarkable electronic properties of two-dimensional van der Waals (vdW) materials make them promising platforms for next-generation spintronic devices. In this study, we demonstrate the room-temperature graphene lateral spin valve devices in the Fe3GaTe2/graphene full vdW heterostructure. The spin transport channel is few-layer graphene, and room-temperature ferromagnet Fe3GaTe2 is used as both the spin injector and detector. Pronounced nonlocal spin valve signals can be observed when the magnetic field sweeps along the out-of-plane easy axis direction of Fe3GaTe2. This nonlocal spin valve signal persists even at 320 K, realizing a room-temperature lateral spin valve in full vdW heterostructure. Additionally, a significant magnitude nonlocal spin valve signal can be detected even with the low bias current of 1 μA. Furthermore, the magnetic field angle-dependent nonlocal measurements revealed that the nonlocal spin valve behavior is closely related to the robust large perpendicular magnetic anisotropy property of Fe3GaTe2. The nonlocal spin valve signal is prominent when the magnetic field is applied near the perpendicular direction and disappears under the in-plane magnetic field. These results demonstrate the potential of Fe3GaTe2 as a prospective candidate for constructing room-temperature, two-dimensional vdW spintronic devices.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00510

Chinese Library Classification Number:

Citation Information:

The remarkable electronic properties of two-dimensional van der Waals (vdW) materials make them promising platforms for next-generation spintronic devices. In this study, we demonstrate the room-temperature graphene lateral spin valve devices in the Fe3GaTe2/graphene full vdW heterostructure. The spin transport channel is few-layer graphene, and room-temperature ferromagnet Fe3GaTe2 is used as both the spin injector and detector. Pronounced nonlocal spin valve signals can be observed when the magnetic field sweeps along the out-of-plane easy axis direction of Fe3GaTe2. This nonlocal spin valve signal persists even at 320 K, realizing a room-temperature lateral spin valve in full vdW heterostructure. Additionally, a significant magnitude nonlocal spin valve signal can be detected even with the low bias current of 1 μA. Furthermore, the magnetic field angle-dependent nonlocal measurements revealed that the nonlocal spin valve behavior is closely related to the robust large perpendicular magnetic anisotropy property of Fe3GaTe2. The nonlocal spin valve signal is prominent when the magnetic field is applied near the perpendicular direction and disappears under the in-plane magnetic field. These results demonstrate the potential of Fe3GaTe2 as a prospective candidate for constructing room-temperature, two-dimensional vdW spintronic devices.

quote

GB/T 7714-2015 [1] Haiyang Pan, Chusheng Zhang, Jiayu Shi, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00510.
MLA [1] Haiyang Pan, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00510.
APA [1] Haiyang Pan, Chusheng Zhang, Jiayu Shi, Xueqi Hu, Naizhou Wang, Liheng An, Ruihuan Duan, Pritam Deb, Zheng Liu, & Weibo Gao. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00510
IEEE [1] Haiyang Pan, Chusheng Zhang, Jiayu Shi, Xueqi Hu, Naizhou Wang, Liheng An, Ruihuan Duan, Pritam Deb, Zheng Liu, and Weibo Gao, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00510.