Polyphosphate-Based Hydrogels as Drug-Loaded Wound Dressing: An In Vitro Study AITranslate

Maastricht University; Maastricht University; Maastricht University; Maastricht University; Maastricht University; Maastricht University; Maastricht University; Maastricht University; Maastricht University; Maastricht University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogels are interesting materials for application in biomedicine due to their outstanding properties (e.g., water retention, drug release, and biocompatibility). This work evaluates two series of phosphorus-based hydrogels as potential wound-dressing candidates. The materials were synthesized via free-radical polymerization of bis[2-(methacryloyloxy)ethyl] phosphate (BMEP, ≥75 wt %) with (3-acrylamidopropyl)trimethylammonium chloride solution (APTAC) or 2-acrylamido-2-methyl-1-propane sulfonic acid (AMPS). Due to optimized synthetic conditions, the materials displayed an unprecedented compressive elastic modulus (E′) reaching up to 0.19 MPa, which represents a 1000-fold increase compared to previously reported materials. Furthermore, the hydrogels displayed good hydrolytic and enzymatic stability, cytocompatibility using bovine fibroblasts (BFs), and drug loading/release in woundlike pH conditions. In summary, this work demonstrates the potential of phosphorus-based hydrogels as drug-eluting wound-dressing materials.

KeyWords AITranslate

poly(phosphodiesters) poly(phosphates) hydrogels wound dressing drug delivery cytocompatibility mechanical properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01533

Chinese Library Classification Number:

Citation Information:

Hydrogels are interesting materials for application in biomedicine due to their outstanding properties (e.g., water retention, drug release, and biocompatibility). This work evaluates two series of phosphorus-based hydrogels as potential wound-dressing candidates. The materials were synthesized via free-radical polymerization of bis[2-(methacryloyloxy)ethyl] phosphate (BMEP, ≥75 wt %) with (3-acrylamidopropyl)trimethylammonium chloride solution (APTAC) or 2-acrylamido-2-methyl-1-propane sulfonic acid (AMPS). Due to optimized synthetic conditions, the materials displayed an unprecedented compressive elastic modulus (E′) reaching up to 0.19 MPa, which represents a 1000-fold increase compared to previously reported materials. Furthermore, the hydrogels displayed good hydrolytic and enzymatic stability, cytocompatibility using bovine fibroblasts (BFs), and drug loading/release in woundlike pH conditions. In summary, this work demonstrates the potential of phosphorus-based hydrogels as drug-eluting wound-dressing materials.

quote

GB/T 7714-2015 [1] Ramiro MarroquinGarcia, Jeroen Royakkers, Mick Gagliardi, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01533.
MLA [1] Ramiro MarroquinGarcia, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01533.
APA [1] Ramiro MarroquinGarcia, Jeroen Royakkers, Mick Gagliardi, Rocio ArreguinCampos, Thomas J. Cleij, Kasper Eersels, Nynke M. S. van den Akker, Daniël G. M. Molin, Bart van Grinsven, & Hanne Diliën. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01533
IEEE [1] Ramiro MarroquinGarcia, Jeroen Royakkers, Mick Gagliardi, Rocio ArreguinCampos, Thomas J. Cleij, Kasper Eersels, Nynke M. S. van den Akker, Daniël G. M. Molin, Bart van Grinsven, and Hanne Diliën, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01533. keywords: {poly(phosphodiesters);poly(phosphates);hydrogels;wound dressing;drug delivery;cytocompatibility;mechanical properties}