daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Machine learning approach for prediction of the grafting yield in radiation-induced graft polymerization AITranslate

National Institutes for Quantum and Radiological Science and Technology; National Institutes for Quantum and Radiological Science and Technology; National Institutes for Quantum and Radiological Science and Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Grafting yields for the radiation-induced graft polymerization of a methacrylate ester monomer to give a polyethylene-coated polypropylene nonwoven fabric were predicted as an objective variable by a machine learning approach. The degrees of grafting were obtained from actual experiments. Monomer structure information, atomic charge information, atomic NMR shift information, and infrared absorption wavenumber information, derived from density functional theory calculations, were adopted as explanatory variables of a grafting yield prediction model. Among machine learning algorithms as a prediction model on the grafting yield, XGBoost and random forest models showed higher prediction accuracy, compared to a multiple linear regression model. The prediction accuracies of the various algorithm decreased in the order: XGBoost > random forest > multiple linear regression/LASSO > decision tree > multiple linear regression. The monomer polarizability and the O2 NMR shift were found to be important explanatory variables for predicting the grafting yield in the XGBoost model. This is probably because the polarizability, which represents a miscibility indicator of the monomer to the trunk polymer, and the O2 NMR shift, which represents a diffusivity indicator of the monomer into the trunk polymer, remarkably reflect the difference in the substituent structure of the methacrylate ester monomers. Graphical abstract Download : Download high-res image (141KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101158

Chinese Library Classification Number:

Citation Information:

Grafting yields for the radiation-induced graft polymerization of a methacrylate ester monomer to give a polyethylene-coated polypropylene nonwoven fabric were predicted as an objective variable by a machine learning approach. The degrees of grafting were obtained from actual experiments. Monomer structure information, atomic charge information, atomic NMR shift information, and infrared absorption wavenumber information, derived from density functional theory calculations, were adopted as explanatory variables of a grafting yield prediction model. Among machine learning algorithms as a prediction model on the grafting yield, XGBoost and random forest models showed higher prediction accuracy, compared to a multiple linear regression model. The prediction accuracies of the various algorithm decreased in the order: XGBoost > random forest > multiple linear regression/LASSO > decision tree > multiple linear regression. The monomer polarizability and the O2 NMR shift were found to be important explanatory variables for predicting the grafting yield in the XGBoost model. This is probably because the polarizability, which represents a miscibility indicator of the monomer to the trunk polymer, and the O2 NMR shift, which represents a diffusivity indicator of the monomer into the trunk polymer, remarkably reflect the difference in the substituent structure of the methacrylate ester monomers. Graphical abstract Download : Download high-res image (141KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Yuji Ueki, Noriaki Seko, Yasunari Maekawa. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101158.
MLA [1] Yuji Ueki, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101158.
APA [1] Yuji Ueki, Noriaki Seko, & Yasunari Maekawa. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101158
IEEE [1] Yuji Ueki, Noriaki Seko, and Yasunari Maekawa, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101158.