Enabling Highly Reversible Zn Anode by Multifunctional Synergistic Effects of Hybrid Solute Additives AITranslate
Abstract AITranslate
Aqueous zinc ion batteries are promising secondary batteries for next-generation electrochemical energy storage. In this work, we report a hybrid electrolyte system with 3 M Zn(OTf)2 as zinc salt and 1 M urea + 0.3 M LiOAc as hybrid solute additives for highly reversible aqueous zinc ion batteries. In this electrolyte system, partial coordinated water molecules of Zn2+ are replaced, and the original hydrogen bond network of the bulk electrolyte also suffers from interruption. Moreover, the introduction of lithium acetate solves the aggravated self-corrosion caused by urea on the one hand and inhibits the growth of dendrites through the electrostatic shielding effect on the other. Benefiting from this multifunctional synergistic effect, dendrite-free Zn plating/stripping for 600 h at 4.8 mA cm–2 (20% depth of discharge) and highly reversible plating/stripping at ∼99.7% Coulombic efficiency with a high cumulative plating capacity of 1600 mAh is achieved.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02455
Chinese Library Classification Number:
Citation Information:
Aqueous zinc ion batteries are promising secondary batteries for next-generation electrochemical energy storage. In this work, we report a hybrid electrolyte system with 3 M Zn(OTf)2 as zinc salt and 1 M urea + 0.3 M LiOAc as hybrid solute additives for highly reversible aqueous zinc ion batteries. In this electrolyte system, partial coordinated water molecules of Zn2+ are replaced, and the original hydrogen bond network of the bulk electrolyte also suffers from interruption. Moreover, the introduction of lithium acetate solves the aggravated self-corrosion caused by urea on the one hand and inhibits the growth of dendrites through the electrostatic shielding effect on the other. Benefiting from this multifunctional synergistic effect, dendrite-free Zn plating/stripping for 600 h at 4.8 mA cm–2 (20% depth of discharge) and highly reversible plating/stripping at ∼99.7% Coulombic efficiency with a high cumulative plating capacity of 1600 mAh is achieved.
quote
| GB/T 7714-2015 | [1] Xiang Feng, Peng Li, Junyi Yin, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02455. |
| MLA | [1] Xiang Feng, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02455. |
| APA | [1] Xiang Feng, Peng Li, Junyi Yin, Zihan Gan, Yuan Gao, Mingyan Li, Yonghong Cheng, Xin Xu, Yaqiong Su, & Shujiang Ding. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02455 |
| IEEE | [1] Xiang Feng, Peng Li, Junyi Yin, Zihan Gan, Yuan Gao, Mingyan Li, Yonghong Cheng, Xin Xu, Yaqiong Su, and Shujiang Ding, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02455. |