Turning Harmful Deposition of Metal Impurities into Activation of Nitrogen-Doped Carbon Catalyst toward Durable Electrochemical CO2 Reduction AITranslate

Korea Institute of Science and Technology; National Institute of Advanced Industrial Science and Technology; Korea Institute of Science and Technology; Korea University; Korea Institute of Science and Technology; Korea Institute of Science and Technology; Gwangju Institute of Science and Technology; Kookmin University; Korea University; Yonsei University; Korea University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Electrochemical CO2 reduction is typically operated under highly refined electrolyte conditions. However, trace amounts of metal impurities exist even in ultrapure electrolyte solutions, causing a fatal deactivation of the catalysts. To address this issue, various efforts have been made to prevent the harmful deposition of metal impurities on the catalyst. Herein, we designed a new system where metal impurities are utilized as activators. We demonstrated “self-activation” of the N-doped carbon catalyst in the presence of Fe impurity with remarkable stability for 120 h. The origin of the self-activation was the selective adsorption of Fe impurity forming highly dispersed Fe sites through Fe–N interactions. The correlations between the self-activation and number of N sites and their moieties were investigated and further generalized into other metals, such as Ni, Zn, and Cu. This novel general strategy has enormous impact on design of durable catalysts for various electrochemical reactions suffering from deactivation by metal impurities.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01581

Chinese Library Classification Number:

Citation Information:

Electrochemical CO2 reduction is typically operated under highly refined electrolyte conditions. However, trace amounts of metal impurities exist even in ultrapure electrolyte solutions, causing a fatal deactivation of the catalysts. To address this issue, various efforts have been made to prevent the harmful deposition of metal impurities on the catalyst. Herein, we designed a new system where metal impurities are utilized as activators. We demonstrated “self-activation” of the N-doped carbon catalyst in the presence of Fe impurity with remarkable stability for 120 h. The origin of the self-activation was the selective adsorption of Fe impurity forming highly dispersed Fe sites through Fe–N interactions. The correlations between the self-activation and number of N sites and their moieties were investigated and further generalized into other metals, such as Ni, Zn, and Cu. This novel general strategy has enormous impact on design of durable catalysts for various electrochemical reactions suffering from deactivation by metal impurities.

quote

GB/T 7714-2015 [1] Chanyeon Kim, YoongKee Choe, Da Hye Won, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01581.
MLA [1] Chanyeon Kim, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01581.
APA [1] Chanyeon Kim, YoongKee Choe, Da Hye Won, Ung Lee, HyungSuk Oh, Dong Ki Lee, Chang Hyuck Choi, Sungho Yoon, Woong Kim, Yun Jeong Hwang, & Byoung Koun Min. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01581
IEEE [1] Chanyeon Kim, YoongKee Choe, Da Hye Won, Ung Lee, HyungSuk Oh, Dong Ki Lee, Chang Hyuck Choi, Sungho Yoon, Woong Kim, Yun Jeong Hwang, and Byoung Koun Min, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01581.