Rational Electrode–Electrolyte Design for Efficient Ammonia Electrosynthesis under Ambient Conditions AITranslate

Monash University; Monash University; Monash University; Monash University; Monash University; King Abdullah University of Science and Technology; King Abdullah University of Science and Technology; Monash University; Monash University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Renewable energy-driven ammonia electrosynthesis by N2 reduction reaction (NRR) at ambient conditions is vital for sustainability of both the global population and energy demand. However, NRR under ambient conditions to date has been plagued with a low yield rate and selectivity (<10%) due to the more favorable hydrogen evolution reaction (HER) in aqueous media. Herein, surface area enhanced α-Fe nanorods grown on carbon fiber paper were used as NRR cathodes in an aprotic fluorinated solvent–ionic liquid mixture. Through this design, significantly enhanced NRR activity with an NH3 yield rate of ∼2.35 × 10–11 mol s–1 cmGSA–2, (3.71 × 10–13 mol s–1 cmECSA–2) and selectivity of ∼32% has been achieved under ambient conditions. This study reveals that the use of hydrophobic fluorinated aprotic electrolyte effectively limits the availability of protons and thus suppresses the competing HER. Therefore, electrode–electrolyte engineering is essential in advancing the NH3 electrosynthesis technology.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00487

Chinese Library Classification Number:

Citation Information:

Renewable energy-driven ammonia electrosynthesis by N2 reduction reaction (NRR) at ambient conditions is vital for sustainability of both the global population and energy demand. However, NRR under ambient conditions to date has been plagued with a low yield rate and selectivity (<10%) due to the more favorable hydrogen evolution reaction (HER) in aqueous media. Herein, surface area enhanced α-Fe nanorods grown on carbon fiber paper were used as NRR cathodes in an aprotic fluorinated solvent–ionic liquid mixture. Through this design, significantly enhanced NRR activity with an NH3 yield rate of ∼2.35 × 10–11 mol s–1 cmGSA–2, (3.71 × 10–13 mol s–1 cmECSA–2) and selectivity of ∼32% has been achieved under ambient conditions. This study reveals that the use of hydrophobic fluorinated aprotic electrolyte effectively limits the availability of protons and thus suppresses the competing HER. Therefore, electrode–electrolyte engineering is essential in advancing the NH3 electrosynthesis technology.

quote

GB/T 7714-2015 [1] Bryan H. R. Suryanto, Colin S. M. Kang, Dabin Wang, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00487.
MLA [1] Bryan H. R. Suryanto, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00487.
APA [1] Bryan H. R. Suryanto, Colin S. M. Kang, Dabin Wang, Changlong Xiao, Fengling Zhou, Luis Miguel Azofra, Luigi Cavallo, Xinyi Zhang, & Douglas R. MacFarlane. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00487
IEEE [1] Bryan H. R. Suryanto, Colin S. M. Kang, Dabin Wang, Changlong Xiao, Fengling Zhou, Luis Miguel Azofra, Luigi Cavallo, Xinyi Zhang, and Douglas R. MacFarlane, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00487.