daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Controlling Morphology and Voltage Loss with Ternary Strategy Triggers Efficient All-Small-Molecule Organic Solar Cells AITranslate

Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; Beijing Institute of Technology; The Hong Kong Polytechnic University; Korea University; Beijing Jiaotong University; Beijing Institute of Technology; Beijing Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, an emerging acceptor L8-BO as the third component was combined with the B1:BO-4Cl system for constructing efficient ternary all-small-molecule organic solar cells (ASM-OSCs). Theoretical, morphological, and crystallographic studies reveal that L8-BO and BO-4Cl possess good compatibility, resulting in alloy-like state formation of two acceptors in ternary blends. The synergistic effect of two acceptors is conducive to forming favorable phase separation and molecular stacking for promoting charge splitting and extraction, which contributes to simultaneously boosting short-circuit current density and fill factor. Furthermore, the alloy-like state of two acceptors and the higher lowest unoccupied molecular orbital energy level of L8-BO assist ternary ASM-OSCs in achieving lower voltage loss with respect to the binary devices. The optimal ternary ASM-OSCs with 20 wt % L8-BO deliver a top-level efficiency of 17.10%. This work demonstrates that not only the morphology but also the voltage loss of the small molecular matrix can be well-manipulated by employing the ternary strategy.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02348

Chinese Library Classification Number:

Citation Information:

Herein, an emerging acceptor L8-BO as the third component was combined with the B1:BO-4Cl system for constructing efficient ternary all-small-molecule organic solar cells (ASM-OSCs). Theoretical, morphological, and crystallographic studies reveal that L8-BO and BO-4Cl possess good compatibility, resulting in alloy-like state formation of two acceptors in ternary blends. The synergistic effect of two acceptors is conducive to forming favorable phase separation and molecular stacking for promoting charge splitting and extraction, which contributes to simultaneously boosting short-circuit current density and fill factor. Furthermore, the alloy-like state of two acceptors and the higher lowest unoccupied molecular orbital energy level of L8-BO assist ternary ASM-OSCs in achieving lower voltage loss with respect to the binary devices. The optimal ternary ASM-OSCs with 20 wt % L8-BO deliver a top-level efficiency of 17.10%. This work demonstrates that not only the morphology but also the voltage loss of the small molecular matrix can be well-manipulated by employing the ternary strategy.

quote

GB/T 7714-2015 [1] Mengyun Jiang, HongFu Zhi, Bao Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02348.
MLA [1] Mengyun Jiang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02348.
APA [1] Mengyun Jiang, HongFu Zhi, Bao Zhang, Chucheng Yang, Asif Mahmood, Miao Zhang, Han Young Woo, Fujun Zhang, JinLiang Wang, & Qiaoshi An. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02348
IEEE [1] Mengyun Jiang, HongFu Zhi, Bao Zhang, Chucheng Yang, Asif Mahmood, Miao Zhang, Han Young Woo, Fujun Zhang, JinLiang Wang, and Qiaoshi An, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02348.