Fabrication of Intrinsic, Elastic, Self-healing, and Luminescent CsPbBr3 Quantum Dot-Polymer Composites via Thiol–Ene Cross-Linking AITranslate
Abstract AITranslate
Here, we offer a straightforward approach for making elastic, self-healing, and light-conversion material, in which CsPbBr3 quantum dots (QDs) form a strong bond with a designed copolymer including elastic behavior based on the mechanical characteristics of polyisoprene and reversible bonding moieties for self-healing function. This designed composite film has highly luminescent and typically elastic properties, including good ultimate strength (∼0.14 N/mm2) and high stretchability (∼486%). The copolymer matrix exhibited excellent compatibility with CsPbBr3 QDs, in which they maintained their uniform distribution within the network after a serial stretching process due to the strong bond between copolymers and CsPbBr3 QDs. Furthermore, the composite film dynamic network is capable of 90% self-healing efficiency at room temperature without the need of any healing stimulus, heat, plasticizer, or solvent. This simple method suggested a relatively easy approach to a stable, elastic, and luminescent CsPbBr3 QD-based composite film that opens up the potential of fully stretchable light conversion material for light-emitting diodes.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01352
Chinese Library Classification Number:
Citation Information:
Here, we offer a straightforward approach for making elastic, self-healing, and light-conversion material, in which CsPbBr3 quantum dots (QDs) form a strong bond with a designed copolymer including elastic behavior based on the mechanical characteristics of polyisoprene and reversible bonding moieties for self-healing function. This designed composite film has highly luminescent and typically elastic properties, including good ultimate strength (∼0.14 N/mm2) and high stretchability (∼486%). The copolymer matrix exhibited excellent compatibility with CsPbBr3 QDs, in which they maintained their uniform distribution within the network after a serial stretching process due to the strong bond between copolymers and CsPbBr3 QDs. Furthermore, the composite film dynamic network is capable of 90% self-healing efficiency at room temperature without the need of any healing stimulus, heat, plasticizer, or solvent. This simple method suggested a relatively easy approach to a stable, elastic, and luminescent CsPbBr3 QD-based composite film that opens up the potential of fully stretchable light conversion material for light-emitting diodes.
quote
| GB/T 7714-2015 | [1] YuChing Hsu, YiHong You, AiNhan AuDuong, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01352. |
| MLA | [1] YuChing Hsu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01352. |
| APA | [1] YuChing Hsu, YiHong You, AiNhan AuDuong, YanShin Huang, YuCheng Chiu, & LiangYih Chen. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01352 |
| IEEE | [1] YuChing Hsu, YiHong You, AiNhan AuDuong, YanShin Huang, YuCheng Chiu, and LiangYih Chen, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01352. keywords: {perovskite;quantum dots;stretch;selfhealing;downconversion} |