Measurement of liquidus in metal-rich region of lanthanoid-oxygen binary systems and the thermodynamic evaluation AITranslate

Tokyo Institute of Technology; Tokyo Institute of Technology; Tokyo Institute of Technology;Collaborative Laboratories for Advanced Decommissioning Science, Japan Atomic Energy Agency; Tokyo Institute of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this study, the solubilities of oxygen in molten La, Gd, Tb, Ho, and Er metals were measured and the oxide phases in equilibrium with each of these lanthanoid metals were identified to systematically determine the liquidus of lanthanoid-oxygen systems in the metal-rich region. The molten lanthanoid metal and lanthanoid oxide pellets were equilibrated at 1573–1873 K and then quenched. The oxygen concentration in the quenched metals was measured using inert gas fusion infrared absorption spectroscopy to determine the oxygen solubilities of molten lanthanoid metals. The crystal structures of the quenched lanthanoid oxide pellets were analyzed using XRD to identify the equilibrium oxide phases, which were identified as the sesquioxides of each lanthanoid element. Furthermore, the Gibbs free energies of the liquid phases of the Ln-O (Ln = La, Pr, Gd, Tb, Dy, Ho, Er) systems were evaluated using the CALPHAD method and thermodynamic software Pandat based on the oxygen solubilities of molten La, Gd, Tb, Ho, and Er metals measured in this study and those of Pr and Dy reported in previous studies.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2023.102636

Chinese Library Classification Number:

Citation Information:

In this study, the solubilities of oxygen in molten La, Gd, Tb, Ho, and Er metals were measured and the oxide phases in equilibrium with each of these lanthanoid metals were identified to systematically determine the liquidus of lanthanoid-oxygen systems in the metal-rich region. The molten lanthanoid metal and lanthanoid oxide pellets were equilibrated at 1573–1873 K and then quenched. The oxygen concentration in the quenched metals was measured using inert gas fusion infrared absorption spectroscopy to determine the oxygen solubilities of molten lanthanoid metals. The crystal structures of the quenched lanthanoid oxide pellets were analyzed using XRD to identify the equilibrium oxide phases, which were identified as the sesquioxides of each lanthanoid element. Furthermore, the Gibbs free energies of the liquid phases of the Ln-O (Ln = La, Pr, Gd, Tb, Dy, Ho, Er) systems were evaluated using the CALPHAD method and thermodynamic software Pandat based on the oxygen solubilities of molten La, Gd, Tb, Ho, and Er metals measured in this study and those of Pr and Dy reported in previous studies.

quote

GB/T 7714-2015 [1] Ryota Nakazawa, Ayumi Itoh, Shintaro Yasui, et al. Calphad, 2023(83). DOI:10.1016/j.calphad.2023.102636.
MLA [1] Ryota Nakazawa, et al., Calphad, no. 83, 2023, https://doi.org/10.1016/j.calphad.2023.102636.
APA [1] Ryota Nakazawa, Ayumi Itoh, Shintaro Yasui, Masaki Kurata, & Yoshinao Kobayashi. (2023). Calphad(83). https://doi.org/10.1016/j.calphad.2023.102636
IEEE [1] Ryota Nakazawa, Ayumi Itoh, Shintaro Yasui, Masaki Kurata, and Yoshinao Kobayashi, Calphad, no. 83, 2023, doi: 10.1016/j.calphad.2023.102636.