Self-assembled nanocomposite hydrogels enhanced by nanoparticles phosphonate-magnesium coordination for bone regeneration AITranslate
Abstract AITranslate
The repair of critical-sized bone defects remains challenging. Natural polysaccharide-based hydrogels (NPHs) have shown great promise for facilitating bone defect healing, but limited by osteogenesis, mechanical strength and stability. Here we prepared a water-soluble methacrylic anhydride-co-phosphate modified chitosan (CSMAP) incorporated MgO nanoparticles to form a pergel, and followed by introduction of acrylamide to construct a double-network hydrogel (CSMAP-MgO). We found that Mg2+ released from CSMAP-MgO hydrogel in a stable and sustained manner in 30 days and the compressive strength was maintained and the compressive modulus was even enhanced during immersion in PBS for 28 days. Moreover, the CSMAP-MgO hydrogel was superior in promoting in vitro calcium phosphate deposition, MC3T3-E1 cell proliferation, osteogenic differentiation, and mineralization compared to Magnesium free groups. At 12 weeks post-implantation into a rat critical-sized calvarial defect, the CSMAP-MgO hydrogel promoted significantly more new bone formation compared to CSMAP and non-treated groups. Thus, the CSMAP-MgO hydrogel has great promising as a bone filling material. Graphical abstract Download : Download high-res image (248KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.apmt.2021.101182
Chinese Library Classification Number:
Citation Information:
The repair of critical-sized bone defects remains challenging. Natural polysaccharide-based hydrogels (NPHs) have shown great promise for facilitating bone defect healing, but limited by osteogenesis, mechanical strength and stability. Here we prepared a water-soluble methacrylic anhydride-co-phosphate modified chitosan (CSMAP) incorporated MgO nanoparticles to form a pergel, and followed by introduction of acrylamide to construct a double-network hydrogel (CSMAP-MgO). We found that Mg2+ released from CSMAP-MgO hydrogel in a stable and sustained manner in 30 days and the compressive strength was maintained and the compressive modulus was even enhanced during immersion in PBS for 28 days. Moreover, the CSMAP-MgO hydrogel was superior in promoting in vitro calcium phosphate deposition, MC3T3-E1 cell proliferation, osteogenic differentiation, and mineralization compared to Magnesium free groups. At 12 weeks post-implantation into a rat critical-sized calvarial defect, the CSMAP-MgO hydrogel promoted significantly more new bone formation compared to CSMAP and non-treated groups. Thus, the CSMAP-MgO hydrogel has great promising as a bone filling material. Graphical abstract Download : Download high-res image (248KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Yingqi Chen, Cairong Li, Zhenming Wang, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101182. |
| MLA | [1] Yingqi Chen, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101182. |
| APA | [1] Yingqi Chen, Cairong Li, Zhenming Wang, Jing Long, Ruiqi Wang, Jin Zhao, Wanze Tang, Yu Zhao, Ling Qin, Songlin Peng, & Yuxiao Lai. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101182 |
| IEEE | [1] Yingqi Chen, Cairong Li, Zhenming Wang, Jing Long, Ruiqi Wang, Jin Zhao, Wanze Tang, Yu Zhao, Ling Qin, Songlin Peng, and Yuxiao Lai, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101182. |