High-content lignin-reinforced poly(butylene adipate-co-terephthalate) (PBAT) biocomposites were successfully constructed by the incorporation of lignin particles into a biodegradable PBAT matrix. The effect of lignin content with and without a chain extender (CE) on the thermal and mechanical properties of the biocomposites was investigated. Although the mechanical properties for all biocomposites showed similar decreases with little influence from the addition of CE, the crystallization temperature increased because of the branching points of the PBAT polymer chain, which serve as heterogeneous nucleating sites for crystallization, and the nucleating effect of the lignin particle. The foamability of the lignin-reinforced PBAT biocomposites, which comprised a chemical blowing agent, azodicarbonamide, and a cross-linking agent, dicumyl peroxide, was studied. Was also studied the process in the presence of azodicarbonamide (chemical blowing agent) and dicumyl peroxide (cross-linking agent). When lignin was added to the PBAT biocomposites at a content of less than 20 wt %, a typical foam structure was detected. After the addition of CE, the lignin-reinforced PBAT biocomposites exhibited a cellular structure for lignin contents below 50 wt %. However, the foam quality of the lignin-reinforced PBAT biocomposites with CE was uniform for lignin contents up to 30 wt %. This high-content lignin-reinforced PBAT biocomposite with a CE should provide cost-effective and sustainable biodegradable foam that can be used for cushioning packaging applications.

KeyWords AITranslate

lignin poly(butylene adipatecoterephthalate) chain extender cushioning packaging foamability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01617

Chinese Library Classification Number:

Citation Information:

High-content lignin-reinforced poly(butylene adipate-co-terephthalate) (PBAT) biocomposites were successfully constructed by the incorporation of lignin particles into a biodegradable PBAT matrix. The effect of lignin content with and without a chain extender (CE) on the thermal and mechanical properties of the biocomposites was investigated. Although the mechanical properties for all biocomposites showed similar decreases with little influence from the addition of CE, the crystallization temperature increased because of the branching points of the PBAT polymer chain, which serve as heterogeneous nucleating sites for crystallization, and the nucleating effect of the lignin particle. The foamability of the lignin-reinforced PBAT biocomposites, which comprised a chemical blowing agent, azodicarbonamide, and a cross-linking agent, dicumyl peroxide, was studied. Was also studied the process in the presence of azodicarbonamide (chemical blowing agent) and dicumyl peroxide (cross-linking agent). When lignin was added to the PBAT biocomposites at a content of less than 20 wt %, a typical foam structure was detected. After the addition of CE, the lignin-reinforced PBAT biocomposites exhibited a cellular structure for lignin contents below 50 wt %. However, the foam quality of the lignin-reinforced PBAT biocomposites with CE was uniform for lignin contents up to 30 wt %. This high-content lignin-reinforced PBAT biocomposite with a CE should provide cost-effective and sustainable biodegradable foam that can be used for cushioning packaging applications.

quote

GB/T 7714-2015 [1] SeoHwa Hong, SeokHo Hwang. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01617.
MLA [1] SeoHwa Hong, and SeokHo Hwang. ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01617.
APA [1] SeoHwa Hong, & SeokHo Hwang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01617
IEEE [1] SeoHwa Hong and SeokHo Hwang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01617. keywords: {lignin;poly(butylene adipatecoterephthalate);chain extender;cushioning packaging;foamability}