Unraveling the Cationic and Anionic Redox Reactions in a Conventional Layered Oxide Cathode AITranslate

Lawrence Berkeley National Laboratory; Lawrence Berkeley National Laboratory; University of California;Shell International Exploration & Production; University of California; Lawrence Berkeley National Laboratory; Lawrence Berkeley National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Increasing interest in high-energy lithium-ion batteries has triggered the demand to clarify the reaction mechanism in battery cathodes during high-potential operation. However, the reaction mechanism often involves both transition-metal and oxygen activities that remain elusive. Here we report a comprehensive study of both cationic and anionic redox mechanisms of LiNiO2 nearly full delithiation. Selection of pure LiNiO2 removes the complication of multiple transition metals. Using combined X-ray absorption spectroscopy, resonant inelastic X-ray scattering, and operando differential electrochemical mass spectrometry, we are able to clarify the redox reactions of transition metals in the bulk and at the surface, reversible lattice oxygen redox, and irreversible oxygen release associated with surface reactions. Many findings presented here bring attention to different types of oxygen activities and metal–oxygen interactions in layered oxides, which are of crucial importance to the advancement of a Ni-rich layered oxide cathode for high capacity and long cycling performance.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b02147

Chinese Library Classification Number:

Citation Information:

Increasing interest in high-energy lithium-ion batteries has triggered the demand to clarify the reaction mechanism in battery cathodes during high-potential operation. However, the reaction mechanism often involves both transition-metal and oxygen activities that remain elusive. Here we report a comprehensive study of both cationic and anionic redox mechanisms of LiNiO2 nearly full delithiation. Selection of pure LiNiO2 removes the complication of multiple transition metals. Using combined X-ray absorption spectroscopy, resonant inelastic X-ray scattering, and operando differential electrochemical mass spectrometry, we are able to clarify the redox reactions of transition metals in the bulk and at the surface, reversible lattice oxygen redox, and irreversible oxygen release associated with surface reactions. Many findings presented here bring attention to different types of oxygen activities and metal–oxygen interactions in layered oxides, which are of crucial importance to the advancement of a Ni-rich layered oxide cathode for high capacity and long cycling performance.

quote

GB/T 7714-2015 [1] Ning Li, Shawn Sallis, Joseph K. Papp, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b02147.
MLA [1] Ning Li, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b02147.
APA [1] Ning Li, Shawn Sallis, Joseph K. Papp, James Wei, Bryan D. McCloskey, Wanli Yang, & Wei Tong. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b02147
IEEE [1] Ning Li, Shawn Sallis, Joseph K. Papp, James Wei, Bryan D. McCloskey, Wanli Yang, and Wei Tong, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b02147.