Studying the Effect of MoO3 in Hole-Conductor-Free Perovskite Solar Cells AITranslate

The Hebrew University of Jerusalem; The Hebrew University of Jerusalem
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Owing to the superior properties of hybrid perovskite, it is possible to avoid some of the selective layers in perovksite solar cells (PSCs). One known example is the so-called hole-conductor-free PSCs, which were discovered at the beginning of the perovskite race. In this work, we introduce a thin MoO3 layer, in HTM-free PSCs, at the perovskite/gold interface in order to investigate its influence on photovoltaic (PV) performance and to study the charge extraction behavior, recombination lifetime, and effect of hysteresis. Charge extraction measurements show that implementing a MoO3 layer results in more charges to be extracted; this is beneficial to its PV performance. Intensity-modulated photovoltage spectroscopy shows two characteristic times at high and low frequency. The high frequency is dependent on light intensity and is related to the charge carrier recombination in the perovskite, whereas the low frequency is independent of light intensity and might be related to ion diffusion. Finally, it was observed that the MoO3 forms a noncontinuous layer on the perovskite surface, which on the one hand improves its PV performance but on the other hand does not provide a physical barrier at this interface. This work provides new insights on HTM-free PSCs and the importance of their interfaces.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01169

Chinese Library Classification Number:

Citation Information:

Owing to the superior properties of hybrid perovskite, it is possible to avoid some of the selective layers in perovksite solar cells (PSCs). One known example is the so-called hole-conductor-free PSCs, which were discovered at the beginning of the perovskite race. In this work, we introduce a thin MoO3 layer, in HTM-free PSCs, at the perovskite/gold interface in order to investigate its influence on photovoltaic (PV) performance and to study the charge extraction behavior, recombination lifetime, and effect of hysteresis. Charge extraction measurements show that implementing a MoO3 layer results in more charges to be extracted; this is beneficial to its PV performance. Intensity-modulated photovoltage spectroscopy shows two characteristic times at high and low frequency. The high frequency is dependent on light intensity and is related to the charge carrier recombination in the perovskite, whereas the low frequency is independent of light intensity and might be related to ion diffusion. Finally, it was observed that the MoO3 forms a noncontinuous layer on the perovskite surface, which on the one hand improves its PV performance but on the other hand does not provide a physical barrier at this interface. This work provides new insights on HTM-free PSCs and the importance of their interfaces.

quote

GB/T 7714-2015 [1] Eytan Avigad, Lioz Etgar. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01169.
MLA [1] Eytan Avigad, and Lioz Etgar. ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01169.
APA [1] Eytan Avigad, & Lioz Etgar. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01169
IEEE [1] Eytan Avigad and Lioz Etgar, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01169.