Department of Mechanical Engineering, Advanced Water Research Lab (AWRL);National Research Council Canada (NRC), Nanotechnology Research Centre; University of Alberta; University of Alberta;National Research Council Canada (NRC), Nanotechnology Research Centre;IBM Almaden Research Center, 650 Harry Road;Department of Mechanical Engineering, Advanced Water Research Lab (AWRL)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Star-shaped block copolymers (SPs), comprising a hydrophobic cross-linked polystyrene (PS) core with extended hydrophilic polyethylene glycol (PEG) arms, showed high promise as a class of branched amphiphilic coating material, since the coatability and antifouling properties of the SPs could be tailored simply by tuning the core and/or arm compositions. However, the complex reaction sequences required for synthesizing SPs have been an obstacle for scale-up and, therefore, their practical applications. Herein, we have developed an SP architecture from an inorganic silica nanoparticle (SiO2NP) core, significantly simplifying the synthesis and enabling scale-up at much lower costs. The pressure-assisted coatability of three SiSPs with three different PEG lengths (i.e., SiSP1, SiSP2, and SiSP3 with 28, 54, and 129 PEGMA repeating units) on polysulfone ultrafiltration membranes was evaluated by scanning electron microscopy (SEM) and contact angle measurement. The SiSPs with medium PEG arm length (i.e., SiSP2 with 54 PEGMA repeating units) demonstrated superior thin-layer coatability and UV-induced stabilization. The protein solution filtration exhibited very low fouling, ca. 3% flux decline ratio (FDR) and ca. 97% flux recovery ratio (FRR), for UV-SiSP2 coated PSF UF membrane compared to significant fouling for pristine membrane (ca. 41% FDR and ca. 71% FRR). The three times enhancement in oleophobicity of the SiSP2 coated membrane has endowed almost seven times improvement in the permeation flux during oil emulsion filtration and 100% FRR contrary to zero flux recovery for pristine membrane. This study offers insights regarding the cost-efficient and facile synthesis of block copolymer nanoarchitecture SiSPs, which has the potential for water purification, lubrication, emulsification, and biomedical applications.

KeyWords AITranslate

Silica nanoparticle core Block copolymers Polystyrene arms Polyethylene glycol Antifouling membranes Oil emulsion and Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01197

Chinese Library Classification Number:

Citation Information:

Star-shaped block copolymers (SPs), comprising a hydrophobic cross-linked polystyrene (PS) core with extended hydrophilic polyethylene glycol (PEG) arms, showed high promise as a class of branched amphiphilic coating material, since the coatability and antifouling properties of the SPs could be tailored simply by tuning the core and/or arm compositions. However, the complex reaction sequences required for synthesizing SPs have been an obstacle for scale-up and, therefore, their practical applications. Herein, we have developed an SP architecture from an inorganic silica nanoparticle (SiO2NP) core, significantly simplifying the synthesis and enabling scale-up at much lower costs. The pressure-assisted coatability of three SiSPs with three different PEG lengths (i.e., SiSP1, SiSP2, and SiSP3 with 28, 54, and 129 PEGMA repeating units) on polysulfone ultrafiltration membranes was evaluated by scanning electron microscopy (SEM) and contact angle measurement. The SiSPs with medium PEG arm length (i.e., SiSP2 with 54 PEGMA repeating units) demonstrated superior thin-layer coatability and UV-induced stabilization. The protein solution filtration exhibited very low fouling, ca. 3% flux decline ratio (FDR) and ca. 97% flux recovery ratio (FRR), for UV-SiSP2 coated PSF UF membrane compared to significant fouling for pristine membrane (ca. 41% FDR and ca. 71% FRR). The three times enhancement in oleophobicity of the SiSP2 coated membrane has endowed almost seven times improvement in the permeation flux during oil emulsion filtration and 100% FRR contrary to zero flux recovery for pristine membrane. This study offers insights regarding the cost-efficient and facile synthesis of block copolymer nanoarchitecture SiSPs, which has the potential for water purification, lubrication, emulsification, and biomedical applications.

quote

GB/T 7714-2015 [1] Muhammad Amirul Islam, JaeYoung Cho, Feng Gao, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01197.
MLA [1] Muhammad Amirul Islam, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01197.
APA [1] Muhammad Amirul Islam, JaeYoung Cho, Feng Gao, Michael J. Serpe, Andrew J. Myles, YoungHye La, & Mohtada Sadrzadeh. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01197
IEEE [1] Muhammad Amirul Islam, JaeYoung Cho, Feng Gao, Michael J. Serpe, Andrew J. Myles, YoungHye La, and Mohtada Sadrzadeh, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01197. keywords: {Silica nanoparticle core;Block copolymers;Polystyrene arms;Polyethylene glycol;Antifouling membranes;Oil emulsion and;Show More}