Catechol-Functionalized Latex Polymers Display Improved Adhesion to Low-Surface-Energy Thermoplastic Polyolefin Substrates AITranslate
Abstract AITranslate
We report the synthesis and characterization of catechol-functionalized film-forming latexes that display excellent adhesion to low-surface-energy polyolefin-based substrates. The aromatic 1,2-diol functional group in catechol derivatives is believed to be responsible for enhancing the adhesion of a variety of polymers to a range of substrates. Here, we describe a postpolymerization modification approach to the design of emulsion polymers with catechol-functionalized side chains. A series of analogous small-molecule reactions, together with latex characterization by infrared (IR) spectroscopy and liquid chromatography (LC) methods, provides evidence for polymer functionalization. Films prepared from catechol-containing latexes displayed remarkable adhesion to challenging, commercially-available thermoplastic polyolefin (TPO) (as determined by a standard ASTM cross-hatch method). We provide evidence that covalent bonding and the unique catechol structure are required to promote adhesion. The catechol-functionalized emulsion polymers reported here represent a new class of functional latex, and this postpolymerization modification approach will present further opportunities to improve, modulate, and control the adhesion of water-borne coatings to a variety of polyolefin-based substrates.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00130
Chinese Library Classification Number:
Citation Information:
We report the synthesis and characterization of catechol-functionalized film-forming latexes that display excellent adhesion to low-surface-energy polyolefin-based substrates. The aromatic 1,2-diol functional group in catechol derivatives is believed to be responsible for enhancing the adhesion of a variety of polymers to a range of substrates. Here, we describe a postpolymerization modification approach to the design of emulsion polymers with catechol-functionalized side chains. A series of analogous small-molecule reactions, together with latex characterization by infrared (IR) spectroscopy and liquid chromatography (LC) methods, provides evidence for polymer functionalization. Films prepared from catechol-containing latexes displayed remarkable adhesion to challenging, commercially-available thermoplastic polyolefin (TPO) (as determined by a standard ASTM cross-hatch method). We provide evidence that covalent bonding and the unique catechol structure are required to promote adhesion. The catechol-functionalized emulsion polymers reported here represent a new class of functional latex, and this postpolymerization modification approach will present further opportunities to improve, modulate, and control the adhesion of water-borne coatings to a variety of polyolefin-based substrates.
quote
| GB/T 7714-2015 | [1] Xiangyi Zhang, Matthew C. D. Carter, Matthew E. Belowich, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00130. |
| MLA | [1] Xiangyi Zhang, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00130. |
| APA | [1] Xiangyi Zhang, Matthew C. D. Carter, Matthew E. Belowich, Grace Wan, Matthew Crimmins, Kenneth B. Laughlin, Ralph C. Even, & Thomas H. Kalantar. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00130 |
| IEEE | [1] Xiangyi Zhang, Matthew C. D. Carter, Matthew E. Belowich, Grace Wan, Matthew Crimmins, Kenneth B. Laughlin, Ralph C. Even, and Thomas H. Kalantar, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00130. keywords: {latex;catechol;dopamine;waterborne coatings;thermoplastic polyolefin;adhesion;postpolymerization functionalization} |