The worldwide outbreak of the coronavirus pandemic (COVID-19) and other emerging infections are difficult and sometimes impossible to treat, making them one of the major public health problems of our time. It is noteworthy that Ag-based semiconductors can help orchestrate several strategies to fight this serious societal issue. In this work, we present the synthesis of α-Ag2WO4, β-Ag2MoO4, and Ag2CrO4 and their immobilization in polypropylene in the amounts of 0.5, 1.0, and 3.0 wt %, respectively. The antimicrobial activity of the composites was investigated against the Gram-negative bacterium Escherichia coli, the Gram-positive bacterium Staphylococcus aureus, and the fungus Candida albicans. The best antimicrobial efficiency was achieved by the composite with α-Ag2WO4, which completely eliminated the microorganisms in up to 4 h of exposure. The composites were also tested for the inhibition of SARS-CoV-2 virus, showing antiviral efficiency higher than 98% in just 10 min. Additionally, we evaluated the stability of the antimicrobial activity, resulting in constant inhibition, even after material aging. The antimicrobial activity of the compounds was attributed to the production of reactive oxygen species by the semiconductors, which can induce high local oxidative stress, causing the death of these microorganisms.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00744
Chinese Library Classification Number:
Citation Information:
The worldwide outbreak of the coronavirus pandemic (COVID-19) and other emerging infections are difficult and sometimes impossible to treat, making them one of the major public health problems of our time. It is noteworthy that Ag-based semiconductors can help orchestrate several strategies to fight this serious societal issue. In this work, we present the synthesis of α-Ag2WO4, β-Ag2MoO4, and Ag2CrO4 and their immobilization in polypropylene in the amounts of 0.5, 1.0, and 3.0 wt %, respectively. The antimicrobial activity of the composites was investigated against the Gram-negative bacterium Escherichia coli, the Gram-positive bacterium Staphylococcus aureus, and the fungus Candida albicans. The best antimicrobial efficiency was achieved by the composite with α-Ag2WO4, which completely eliminated the microorganisms in up to 4 h of exposure. The composites were also tested for the inhibition of SARS-CoV-2 virus, showing antiviral efficiency higher than 98% in just 10 min. Additionally, we evaluated the stability of the antimicrobial activity, resulting in constant inhibition, even after material aging. The antimicrobial activity of the compounds was attributed to the production of reactive oxygen species by the semiconductors, which can induce high local oxidative stress, causing the death of these microorganisms.
quote
| GB/T 7714-2015 | [1] Marcelo Assis, Lara K. Ribeiro, Mariana O. Gonçalves, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00744. |
| MLA | [1] Marcelo Assis, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00744. |
| APA | [1] Marcelo Assis, Lara K. Ribeiro, Mariana O. Gonçalves, Lucas H. Staffa, Robert S. Paiva, Lais R. Lima, Dyovani Coelho, Lauana F. Almeida, Leonardo N. Moraes, Ieda L. V. Rosa, Lucia H. Mascaro, Rejane M. T. Grotto, Cristina P. Sousa, Juan Andrés, Elson Longo, & Sandra A. Cruz. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00744 |
| IEEE | [1] Marcelo Assis, Lara K. Ribeiro, Mariana O. Gonçalves, Lucas H. Staffa, Robert S. Paiva, Lais R. Lima, Dyovani Coelho, Lauana F. Almeida, Leonardo N. Moraes, Ieda L. V. Rosa, Lucia H. Mascaro, Rejane M. T. Grotto, Cristina P. Sousa, Juan Andrés, Elson Longo, and Sandra A. Cruz, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00744. keywords: {composites;αAg2WO4;βAg2MoO4;Ag2CrO4;antimicrobial material;antiSARSCoV2 material} |