Polyamine–Diazirine Conjugates for Use as Primers in UHMWPE–Epoxy Composite Materials AITranslate
Abstract AITranslate
Ultra-high-molecular weight polyethylene (UHMWPE) fibers show promise for use in fiber-reinforced polymer composites but have poor interfacial adhesion to the epoxy resin that would serve as the polymer matrix. Here, we describe the development of a diazirine-grafted polyamine that can be used as a topically applied primer for UHMWPE fibers. Activation of the diazirine groups on the primer initiates C–H bond insertion on the polyethylene fiber, leading to strong covalent bonds between the fiber and the polyamine coating. The covalently functionalized surface can then engage in nucleophilic addition reactions with epoxy resin─resulting in increased bonding to the epoxy matrix (demonstrated through lap-shear experiments) and increased performance for fiber-reinforced composite materials (demonstrated through lamination rates and short-beam stress measurements).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01577
Chinese Library Classification Number:
Citation Information:
Ultra-high-molecular weight polyethylene (UHMWPE) fibers show promise for use in fiber-reinforced polymer composites but have poor interfacial adhesion to the epoxy resin that would serve as the polymer matrix. Here, we describe the development of a diazirine-grafted polyamine that can be used as a topically applied primer for UHMWPE fibers. Activation of the diazirine groups on the primer initiates C–H bond insertion on the polyethylene fiber, leading to strong covalent bonds between the fiber and the polyamine coating. The covalently functionalized surface can then engage in nucleophilic addition reactions with epoxy resin─resulting in increased bonding to the epoxy matrix (demonstrated through lap-shear experiments) and increased performance for fiber-reinforced composite materials (demonstrated through lamination rates and short-beam stress measurements).
quote
| GB/T 7714-2015 | [1] Rashid Nazir, Liting Bi, Stefania F. Musolino, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01577. |
| MLA | [1] Rashid Nazir, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01577. |
| APA | [1] Rashid Nazir, Liting Bi, Stefania F. Musolino, Olivia H. Margoto, Kuthan Çelebi, Christophe Mobuchon, Mahdi Takaffoli, Abbas S. Milani, Greg Falck, & Jeremy E. Wulff. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01577 |
| IEEE | [1] Rashid Nazir, Liting Bi, Stefania F. Musolino, Olivia H. Margoto, Kuthan Çelebi, Christophe Mobuchon, Mahdi Takaffoli, Abbas S. Milani, Greg Falck, and Jeremy E. Wulff, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01577. keywords: {polymer composites;UHMWPE;diazirines;crosslinking;primers} |