Facile Fabrication of Amorphous Colloidal Array Patterns with Good Mechanical Stability via an Infiltration-Driven Mayer Rod Coating Method AITranslate

Hangzhou Dianzi University; Hangzhou Dianzi University; Zhejiang Sci-Tech University; Foshan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this study, cationic monodisperse polystyrene (PS) microspheres and polybutyl acrylate (PBA) nanoparticles were synthesized and used in combination to fabricate various steady amorphous colloidal array (ACA) patterns via an infiltration-driven Mayer rod coating method. During the rapid assembly process, PBA nanoparticles were embedded in PS microsphere voids to lock the colloidal array, thereby promoting its mechanical stability. Meanwhile, the fabricated ACA patterns could still exhibit bright angle-independent structural color when moderate PBA nanoparticles introduced. In summary, this study provides a convenient and fast method to fabricate steady ACA patterns, which is a promising potential substitute for traditional ink printing.

KeyWords AITranslate

amorphous colloidal array structural color mechanical stability polystyrene microsphere polybutyl acrylate nanoparticle
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01758

Chinese Library Classification Number:

Citation Information:

In this study, cationic monodisperse polystyrene (PS) microspheres and polybutyl acrylate (PBA) nanoparticles were synthesized and used in combination to fabricate various steady amorphous colloidal array (ACA) patterns via an infiltration-driven Mayer rod coating method. During the rapid assembly process, PBA nanoparticles were embedded in PS microsphere voids to lock the colloidal array, thereby promoting its mechanical stability. Meanwhile, the fabricated ACA patterns could still exhibit bright angle-independent structural color when moderate PBA nanoparticles introduced. In summary, this study provides a convenient and fast method to fabricate steady ACA patterns, which is a promising potential substitute for traditional ink printing.

quote

GB/T 7714-2015 [1] Ting Lü, Jujun Chen, Dongming Qi, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01758.
MLA [1] Ting Lü, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01758.
APA [1] Ting Lü, Jujun Chen, Dongming Qi, & Hongting Zhao. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01758
IEEE [1] Ting Lü, Jujun Chen, Dongming Qi, and Hongting Zhao, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01758. keywords: {amorphous colloidal array;structural color;mechanical stability;polystyrene microsphere;polybutyl acrylate nanoparticle}