Poly(ethylene glycol)-Based Poly(ionic liquid) Block Copolymers through 1,2,3-Triazole Click Reactions AITranslate
Abstract AITranslate
1,2,3-Triazolium-based polyionic liquids (PILs) were made by a copper-catalyzed azide–alkyne cycloaddition (CuAAC) “click” reaction from poly(4-vinylbenzyl chloride). The click reaction facilitates the design and manipulation of the polymer architecture by selecting the desired alkynes, the azide-containing moieties, and the alkylating group of the 1,2,3-triazole group. Using this versatile chemistry and design, we prepared PILs with comblike homo- and block copolymer architectures using bistrifluoromethanesulfonimidate (TFSI-) as counterions. The block copolymer self-assembles into an ordered morphology. The block copolymer was integrated into metal–insulator–metal capacitors and found to display a prominent electrical double layer when characterized by electrochemical impedance spectroscopy.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01678
Chinese Library Classification Number:
Citation Information:
1,2,3-Triazolium-based polyionic liquids (PILs) were made by a copper-catalyzed azide–alkyne cycloaddition (CuAAC) “click” reaction from poly(4-vinylbenzyl chloride). The click reaction facilitates the design and manipulation of the polymer architecture by selecting the desired alkynes, the azide-containing moieties, and the alkylating group of the 1,2,3-triazole group. Using this versatile chemistry and design, we prepared PILs with comblike homo- and block copolymer architectures using bistrifluoromethanesulfonimidate (TFSI-) as counterions. The block copolymer self-assembles into an ordered morphology. The block copolymer was integrated into metal–insulator–metal capacitors and found to display a prominent electrical double layer when characterized by electrochemical impedance spectroscopy.
quote
| GB/T 7714-2015 | [1] Jukka Niskanen, Mathieu N. Tousignant, Alexander J. Peltekoff, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01678. |
| MLA | [1] Jukka Niskanen, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01678. |
| APA | [1] Jukka Niskanen, Mathieu N. Tousignant, Alexander J. Peltekoff, & Benoît H. Lessard. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01678 |
| IEEE | [1] Jukka Niskanen, Mathieu N. Tousignant, Alexander J. Peltekoff, and Benoît H. Lessard, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01678. keywords: {1;2;3triazolium;poly(ionic liquid)s;coppercatalyzed azide−alkyne cycloaddition;capacitor;conductivity;block copolymer;Show More} |