daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Solvent-Engineered Design of Argyrodite Li6PS5X (X = Cl, Br, I) Solid Electrolytes with High Ionic Conductivity AITranslate

200 University Avenue West; 200 University Avenue West; 200 University Avenue West; 200 University Avenue West;BASF SE, Ludwigshafen 67063;BASF SE, Ludwigshafen 67063; 200 University Avenue West
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Argyrodites, Li6PS5X (X = Cl, Br), are considered to be one of the most promising solid-state electrolytes for solid-state batteries. However, while traditional ball-mill approaches to prepare these materials do not promote scale-up, solution-based preparative methods have resulted in poor ionic conductivity. Herein, we report a solution-engineered, scalable approach to these materials, including the new argyrodite solid solution phase Li6–yPS5–yCl1+y (y = 0–0.5), that shows very high ionic conductivities (up to 3.9 mS·cm–1) and negligible electronic conductivities. These properties are almost the same as their analogues prepared by solid-state methods, owing to a lack of amorphous contributions and low impurity contents ranging from 3 to 10%. Electrochemical performance is demonstrated for Li6PS5Cl in a prototype solid-state battery and compared to that of the same solid electrolyte derived from classic ball-milling processing.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01997

Chinese Library Classification Number:

Citation Information:

Argyrodites, Li6PS5X (X = Cl, Br), are considered to be one of the most promising solid-state electrolytes for solid-state batteries. However, while traditional ball-mill approaches to prepare these materials do not promote scale-up, solution-based preparative methods have resulted in poor ionic conductivity. Herein, we report a solution-engineered, scalable approach to these materials, including the new argyrodite solid solution phase Li6–yPS5–yCl1+y (y = 0–0.5), that shows very high ionic conductivities (up to 3.9 mS·cm–1) and negligible electronic conductivities. These properties are almost the same as their analogues prepared by solid-state methods, owing to a lack of amorphous contributions and low impurity contents ranging from 3 to 10%. Electrochemical performance is demonstrated for Li6PS5Cl in a prototype solid-state battery and compared to that of the same solid electrolyte derived from classic ball-milling processing.

quote

GB/T 7714-2015 [1] Laidong Zhou, KernHo Park, Xiaoqi Sun, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b01997.
MLA [1] Laidong Zhou, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b01997.
APA [1] Laidong Zhou, KernHo Park, Xiaoqi Sun, Fabien Lalère, Torben Adermann, Pascal Hartmann, & Linda F. Nazar. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b01997
IEEE [1] Laidong Zhou, KernHo Park, Xiaoqi Sun, Fabien Lalère, Torben Adermann, Pascal Hartmann, and Linda F. Nazar, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b01997.