Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School; Peking University Shenzhen Graduate School
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metallic Zn anodes exhibit uncontrollable dendrites, impractically low Zn utilization, hydrogen evolution, and unexpected byproducts, limiting the practical process of aqueous zinc-ion batteries (AZIBs); thus, exploring alternative insertion anodes has become a reasonable strategy, exemplified by the successful application of graphite anodes in lithium-ion batteries. However, the current intercalative anodes are still plagued by high Zn2+ insertion potential and inadequate cycle life, and the alternative choice is quite limited. Here, we report a polyanionic insertion anode (Ti2O(PO4)2·2H2O) that shows an extremely low insertion potential of 0.07 V with a reversible capacity of 124.6 mAh g–1. This anode possesses a robust and spacious framework, demonstrating high reversibility with low strain during cycling. Coupled with a KZnHCF cathode, a 1.6 V “rocking-chair” full battery is achieved with an ultralong life of 5000 cycles, surpassing the reported congeneric batteries. This work shares a new vision for the development of practical AZIBs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00985

Chinese Library Classification Number:

Citation Information:

Metallic Zn anodes exhibit uncontrollable dendrites, impractically low Zn utilization, hydrogen evolution, and unexpected byproducts, limiting the practical process of aqueous zinc-ion batteries (AZIBs); thus, exploring alternative insertion anodes has become a reasonable strategy, exemplified by the successful application of graphite anodes in lithium-ion batteries. However, the current intercalative anodes are still plagued by high Zn2+ insertion potential and inadequate cycle life, and the alternative choice is quite limited. Here, we report a polyanionic insertion anode (Ti2O(PO4)2·2H2O) that shows an extremely low insertion potential of 0.07 V with a reversible capacity of 124.6 mAh g–1. This anode possesses a robust and spacious framework, demonstrating high reversibility with low strain during cycling. Coupled with a KZnHCF cathode, a 1.6 V “rocking-chair” full battery is achieved with an ultralong life of 5000 cycles, surpassing the reported congeneric batteries. This work shares a new vision for the development of practical AZIBs.

quote

GB/T 7714-2015 [1] Wenjun Deng, Zhongyuan Huang, Zhuqing Zhou, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00985.
MLA [1] Wenjun Deng, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00985.
APA [1] Wenjun Deng, Zhongyuan Huang, Zhuqing Zhou, Chang Li, Yan Chen, Yi Zhou, Chao Huang, Jinlin Zhu, Wenxia Zou, Runduo Zhu, Yushuang Xu, & Rui Li. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00985
IEEE [1] Wenjun Deng, Zhongyuan Huang, Zhuqing Zhou, Chang Li, Yan Chen, Yi Zhou, Chao Huang, Jinlin Zhu, Wenxia Zou, Runduo Zhu, Yushuang Xu, and Rui Li, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00985.