Quaternary Ammonium-Functionalized Polyethylene-Based Anion Exchange Membranes: Balancing Performance and Stability AITranslate

Cornell University; Cornell University; Cornell University; Cornell University; Cornell University; Cornell University; Cornell University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Anion exchange membrane water electrolyzers (AEMWEs) and fuel cells (AEMFCs) require an anion exchange membrane (AEM) with high hydroxide ion conductivity and high chemical stability to oxidative and alkaline conditions. Herein the conductivities of 17 quaternary ammonium-functionalized polyethylene-based AEMs were measured over time to understand the influence of ammonium functional groups on AEM performance. The piperidinium-based AEM containing a β-methyl in the backbone resulted in a hydroxide conductivity of 41 mS/cm at 22 °C and the highest stability with a 95% conductivity retention after 30 days in 1 M KOH at 80 °C. In fuel cell tests, increasing the ion exchange capacity of the piperidinium-based AEM led to increased performance from a peak power density of 0.7 to 1.0 W/cm2, enabling it to compete with other state-of-the-art AEMs after optimization.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00319

Chinese Library Classification Number:

Citation Information:

Anion exchange membrane water electrolyzers (AEMWEs) and fuel cells (AEMFCs) require an anion exchange membrane (AEM) with high hydroxide ion conductivity and high chemical stability to oxidative and alkaline conditions. Herein the conductivities of 17 quaternary ammonium-functionalized polyethylene-based AEMs were measured over time to understand the influence of ammonium functional groups on AEM performance. The piperidinium-based AEM containing a β-methyl in the backbone resulted in a hydroxide conductivity of 41 mS/cm at 22 °C and the highest stability with a 95% conductivity retention after 30 days in 1 M KOH at 80 °C. In fuel cell tests, increasing the ion exchange capacity of the piperidinium-based AEM led to increased performance from a peak power density of 0.7 to 1.0 W/cm2, enabling it to compete with other state-of-the-art AEMs after optimization.

quote

GB/T 7714-2015 [1] Cheyenne R. Peltier, Wei You, Dea Fackovic Volcanjk, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00319.
MLA [1] Cheyenne R. Peltier, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00319.
APA [1] Cheyenne R. Peltier, Wei You, Dea Fackovic Volcanjk, Qihao Li, Alexandra J. Macbeth, Héctor D. Abruña, & Geoffrey W. Coates. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00319
IEEE [1] Cheyenne R. Peltier, Wei You, Dea Fackovic Volcanjk, Qihao Li, Alexandra J. Macbeth, Héctor D. Abruña, and Geoffrey W. Coates, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00319.