daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Residual Pd Enables Photocatalytic H2 Evolution from Conjugated Polymers AITranslate

Department of Physical Sciences and Engineering, KAUST Solar Centre (KSC); Imperial College London
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01853

Chinese Library Classification Number:

Citation Information:

quote

GB/T 7714-2015 [1] Jan Kosco, Iain McCulloch. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01853.
MLA [1] Jan Kosco, and Iain McCulloch. ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01853.
APA [1] Jan Kosco, & Iain McCulloch. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01853
IEEE [1] Jan Kosco and Iain McCulloch, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01853.