Solar Photocatalytic Phenol Polymerization and Hydrogen Generation for Flocculation of Wastewater Impurities AITranslate

University of Colorado; University of Colorado; University of Colorado; University of Colorado; University of Colorado; University of Colorado; University of Colorado
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Achieving global sustainability will require balancing encroaching climate changes while maintaining the existing quality of life. Using sunlight to purify wastewater while simultaneously generating usable fuels is an opportunity to approach both targets in a cost-efficient manner. In addition, converting biomass products to usable polymers is a sustainable approach for potentially replacing polystyrene or other petroleum-derived polymers. Phenols from medical, manufacturing, and agricultural waste are commonly found in many water sources, and they are known to foul common reverse osmosis membranes. Here, we show oxidative polymerization of guaiacol, an aromatic compound derived from biomass, with concurrent hydrogen gas generation by using platinum-seeded cadmium sulfide nanorods (Pt@CdS) as photocatalysts. Rather than forming short oligomers as typically made by enzymes such as laccase and peroxidase, the resulting polymers show higher molecular weights that can more easily flocculate out of water. By comparing guaiacol conversion to molecular weight and dispersity, we found the guaiacol to polymerize via a chain-growth process. We also show that Pt@CdS can polymerize other phenols as well by testing the monomers phenol, 2,6-dihydroxybenzoic acid, gallic acid, and vanillin. Lastly, because the aqueous solubility of these aromatic polymers decreases dramatically with molecular weight, polymerization reactions were also tested in biphasic solutions to determine whether chain growth could propagate in the oil phase. We show that the Pt@CdS nanoparticles can form stable Pickering emulsions in various biphasic combinations and that both H2 formation and polymer molecular weight correlated to the partition coefficient of guaiacol into the oil phase as well as the solubility of the growing polymer chains. These combined studies demonstrate the possibility of using nanoscale photocatalysts to oxidatively polymerize phenolic substrates via a chain-growth mechanism, thereby providing a path for pretreating water by flocculating out contaminants with concurrent generation of hydrogen.

KeyWords AITranslate

photocatalysis phenol polymerization green chemistry wastewater purification biphasic systems
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00210

Chinese Library Classification Number:

Citation Information:

Achieving global sustainability will require balancing encroaching climate changes while maintaining the existing quality of life. Using sunlight to purify wastewater while simultaneously generating usable fuels is an opportunity to approach both targets in a cost-efficient manner. In addition, converting biomass products to usable polymers is a sustainable approach for potentially replacing polystyrene or other petroleum-derived polymers. Phenols from medical, manufacturing, and agricultural waste are commonly found in many water sources, and they are known to foul common reverse osmosis membranes. Here, we show oxidative polymerization of guaiacol, an aromatic compound derived from biomass, with concurrent hydrogen gas generation by using platinum-seeded cadmium sulfide nanorods (Pt@CdS) as photocatalysts. Rather than forming short oligomers as typically made by enzymes such as laccase and peroxidase, the resulting polymers show higher molecular weights that can more easily flocculate out of water. By comparing guaiacol conversion to molecular weight and dispersity, we found the guaiacol to polymerize via a chain-growth process. We also show that Pt@CdS can polymerize other phenols as well by testing the monomers phenol, 2,6-dihydroxybenzoic acid, gallic acid, and vanillin. Lastly, because the aqueous solubility of these aromatic polymers decreases dramatically with molecular weight, polymerization reactions were also tested in biphasic solutions to determine whether chain growth could propagate in the oil phase. We show that the Pt@CdS nanoparticles can form stable Pickering emulsions in various biphasic combinations and that both H2 formation and polymer molecular weight correlated to the partition coefficient of guaiacol into the oil phase as well as the solubility of the growing polymer chains. These combined studies demonstrate the possibility of using nanoscale photocatalysts to oxidatively polymerize phenolic substrates via a chain-growth mechanism, thereby providing a path for pretreating water by flocculating out contaminants with concurrent generation of hydrogen.

quote

GB/T 7714-2015 [1] Glenn R. Hafenstine, Ryan E. Patalano, Alexander W. Harris, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00210.
MLA [1] Glenn R. Hafenstine, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00210.
APA [1] Glenn R. Hafenstine, Ryan E. Patalano, Alexander W. Harris, Grace Jiang, Ke Ma, Andrew P. Goodwin, & Jennifer N. Cha. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00210
IEEE [1] Glenn R. Hafenstine, Ryan E. Patalano, Alexander W. Harris, Grace Jiang, Ke Ma, Andrew P. Goodwin, and Jennifer N. Cha, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00210. keywords: {photocatalysis;phenol polymerization;green chemistry;wastewater purification;biphasic systems}