daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Water-Soluble Napthalimide-Conjugated N-Nitrosamine-Based Block Copolymers for Photoinduced Nitric Oxide Delivery and Cell Imaging AITranslate

Indian Institute of Science Education and Research Kolkata; Indian Institute of Science Education and Research Kolkata; Indian Institute of Science Education and Research Kolkata; Indian Institute of Science Education and Research Kolkata; Indian Institute of Science Education and Research Kolkata; Indian Institute of Science Education and Research Kolkata
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

N-Nitrosamine-derived nitric oxide (NO) delivery agents find widespread use in diverse biomedical applications, including cancer therapy. To understand how NO is released from these compounds and acts within cells, herein, we report a facile approach to synthesize N-nitrosamine-bound water-soluble napthalimide-based block copolymers (BCPx-NO) with improved regulation over their molecular weight and aqueous solution self-assembly. These polymers exhibit a fluorescence “turn-on” response upon photostimulated (365 nm, 3.71 mW/cm2) NO release, delivering 47–53 μM of NO within 10 h, while their concentration varied from 0.26 to 0.60 mg/mL. This accounts for approximately 67–75% of the theoretically bound NO within the polymers. The fluorescence “turn-on” response is characteristic of the small-molecule NO donor (NOD), although the emission time has a longer half-life in the polymers. The type of NO released from the NOD is a nitric oxide radical (•NO), as per the electron paramagnetic resonance spectroscopy results. The in vitro NO release in response to the photoirradiation and the consequent acquired fluorescence are corroborated using flow cytometry and confocal imaging studies. It was also manifested that these NO conjugated polymers can physically encapsulate doxorubicin (DOX) in aqueous environment, and the synergistic effect of DOX and NO is reflected in the exhibited cytotoxicity against the MCF-7 (human breast adenocarcinoma) cells. The spatiotemporally modulated NO release steered fluorescence “turn-on” may find abundant biomedical applications.

KeyWords AITranslate

nitric oxide (NO) block copolymer Nnitrosamine phototrigger fluorogenic response
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02759

Chinese Library Classification Number:

Citation Information:

N-Nitrosamine-derived nitric oxide (NO) delivery agents find widespread use in diverse biomedical applications, including cancer therapy. To understand how NO is released from these compounds and acts within cells, herein, we report a facile approach to synthesize N-nitrosamine-bound water-soluble napthalimide-based block copolymers (BCPx-NO) with improved regulation over their molecular weight and aqueous solution self-assembly. These polymers exhibit a fluorescence “turn-on” response upon photostimulated (365 nm, 3.71 mW/cm2) NO release, delivering 47–53 μM of NO within 10 h, while their concentration varied from 0.26 to 0.60 mg/mL. This accounts for approximately 67–75% of the theoretically bound NO within the polymers. The fluorescence “turn-on” response is characteristic of the small-molecule NO donor (NOD), although the emission time has a longer half-life in the polymers. The type of NO released from the NOD is a nitric oxide radical (•NO), as per the electron paramagnetic resonance spectroscopy results. The in vitro NO release in response to the photoirradiation and the consequent acquired fluorescence are corroborated using flow cytometry and confocal imaging studies. It was also manifested that these NO conjugated polymers can physically encapsulate doxorubicin (DOX) in aqueous environment, and the synergistic effect of DOX and NO is reflected in the exhibited cytotoxicity against the MCF-7 (human breast adenocarcinoma) cells. The spatiotemporally modulated NO release steered fluorescence “turn-on” may find abundant biomedical applications.

quote

GB/T 7714-2015 [1] Soumya Paul, Shilpendu Ghosh, Manish Kumar, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02759.
MLA [1] Soumya Paul, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02759.
APA [1] Soumya Paul, Shilpendu Ghosh, Manish Kumar, Tanmoy Maity, Arindam Mukherjee, & Priyadarsi De. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02759
IEEE [1] Soumya Paul, Shilpendu Ghosh, Manish Kumar, Tanmoy Maity, Arindam Mukherjee, and Priyadarsi De, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02759. keywords: {nitric oxide (NO);block copolymer;Nnitrosamine;phototrigger;fluorogenic response}