Differentiating between Ion Transport and Plating–Stripping Phenomena in Magnesium Battery Electrolytes Using Operando Raman Spectroscopy AITranslate

University of Strathclyde;National Physical Laboratory; University of Strathclyde; University of Strathclyde;National Physical Laboratory;National Physical Laboratory;National Physical Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Understanding metal plating–stripping and mass transport processes is necessary for the development of new electrolytes for post-lithium energy storage applications. Operando vibrational spectroscopy is a valuable analytical tool for this purpose, enabling structural and chemical changes at electrode–electrolyte interfaces to be probed dynamically, under battery cycling conditions. In this work we apply operando Raman spectroscopy to characterize the behavior of the Mg based “all phenyl complex” [Mg2Cl3]+[AlPh4]− in tetrahydrofuran (THF), an exemplar electrolyte for emerging Mg battery technologies. We demonstrate that the observed electrolyte Raman band intensities vary reversibly with electrochemical cycling due to anion migration in response to the applied electric field, while Mg plating and stripping can be monitored independently through the broad background scattering intensity. Spectral measurements across different sites of the platinum working electrode indicate that the ion transport response is spatially heterogeneous, while the plating and stripping response is ubiquitous.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00279

Chinese Library Classification Number:

Citation Information:

Understanding metal plating–stripping and mass transport processes is necessary for the development of new electrolytes for post-lithium energy storage applications. Operando vibrational spectroscopy is a valuable analytical tool for this purpose, enabling structural and chemical changes at electrode–electrolyte interfaces to be probed dynamically, under battery cycling conditions. In this work we apply operando Raman spectroscopy to characterize the behavior of the Mg based “all phenyl complex” [Mg2Cl3]+[AlPh4]− in tetrahydrofuran (THF), an exemplar electrolyte for emerging Mg battery technologies. We demonstrate that the observed electrolyte Raman band intensities vary reversibly with electrochemical cycling due to anion migration in response to the applied electric field, while Mg plating and stripping can be monitored independently through the broad background scattering intensity. Spectral measurements across different sites of the platinum working electrode indicate that the ion transport response is spatially heterogeneous, while the plating and stripping response is ubiquitous.

quote

GB/T 7714-2015 [1] Rudra N. Samajdar, Sofia Marchesini, Scott A. Brown, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00279.
MLA [1] Rudra N. Samajdar, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00279.
APA [1] Rudra N. Samajdar, Sofia Marchesini, Scott A. Brown, Stuart D. Robertson, Keith R. Paton, Andrew J. Pollard, & Andrew J. Wain. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00279
IEEE [1] Rudra N. Samajdar, Sofia Marchesini, Scott A. Brown, Stuart D. Robertson, Keith R. Paton, Andrew J. Pollard, and Andrew J. Wain, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00279.