Power Conversion Efficiency Enhancement of Low-Bandgap Mixed Pb–Sn Perovskite Solar Cells by Improved Interfacial Charge Transfer AITranslate
Abstract AITranslate
The power conversion efficiency (PCE) of low-bandgap mixed Pb–Sn perovskite solar cells (PSCs) has been significantly hindered by large open-circuit voltage (Voc) loss and poor fill factor (FF). Herein, mixed Pb–Sn perovskite films with a composition (FASnI3)0.6(MAPbI3)0.4 were processed with a simple delayed annealing (DA) treatment that enables perovskite films with significantly reduced surface roughness. The treatment reduces nonradiative recombination of interfacial contacts when the perovskite films are interfaced with poly(3,4-ethylenedioxythiphene):poly(styrenesulfonate) (PEDOT:PSS) and fullerene (C60). Charge transfer at the carrier-collection interfaces has been effectively improved, in agreement with time-resolved photoluminescence (TRPL) and transient photovoltage/photocurrent results. Consequently, the champion cell based on perovskite films with DA treatment shows a high Voc of 0.824 V, indicating a greatly suppressed Voc loss (for a bandgap of ∼1.25 eV), and an overall PCE of over 18.6%.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00880
Chinese Library Classification Number:
Citation Information:
The power conversion efficiency (PCE) of low-bandgap mixed Pb–Sn perovskite solar cells (PSCs) has been significantly hindered by large open-circuit voltage (Voc) loss and poor fill factor (FF). Herein, mixed Pb–Sn perovskite films with a composition (FASnI3)0.6(MAPbI3)0.4 were processed with a simple delayed annealing (DA) treatment that enables perovskite films with significantly reduced surface roughness. The treatment reduces nonradiative recombination of interfacial contacts when the perovskite films are interfaced with poly(3,4-ethylenedioxythiphene):poly(styrenesulfonate) (PEDOT:PSS) and fullerene (C60). Charge transfer at the carrier-collection interfaces has been effectively improved, in agreement with time-resolved photoluminescence (TRPL) and transient photovoltage/photocurrent results. Consequently, the champion cell based on perovskite films with DA treatment shows a high Voc of 0.824 V, indicating a greatly suppressed Voc loss (for a bandgap of ∼1.25 eV), and an overall PCE of over 18.6%.
quote
| GB/T 7714-2015 | [1] Tingming Jiang, Zeng Chen, Xu Chen, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00880. |
| MLA | [1] Tingming Jiang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00880. |
| APA | [1] Tingming Jiang, Zeng Chen, Xu Chen, Xinya Chen, Xuehui Xu, Tianyu Liu, Lizhong Bai, Dexin Yang, Dawei Di, Wei E. I. Sha, Haiming Zhu, & Yang Michael Yang. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00880 |